Abstract The nucleation of boride at boronizing initiation and the microstruc-tural difference in the boride crystals at different stages of growth have been observedunder TEM by using the single-side thinning technique. It seems that the controllingfactors proposed in growth of boronizing layer are the density of nuclei of botidecrystals on the surface of specimen. The process of boronizing may be described bytwo stages. First, the layer will thicken as the time prolonged according to a parabo-lic growth. Until the compressive stress in the front of layer is increased over a cer-tain critic value, the stacking faults will be induced in the boride crystals, so as toacceralate the diffusion of boron atoms and the growth of layer. This is called thesecond stage. In this stage, the deviation from parabolic growth and the approach toa straigh line relationship would be revealed.
|
|
Received: 18 January 1991
|
1 林振湛,卢光熙.金属热处理学报,1983;4(2) : 38 2 陆明炯.西德的固体渗硼,上海材料研究所内部资料,1983 3 蒋百灵.哈尔滨工业大学博士学位论文,1989 4 孙喜臣.金属科学与工艺,1988;(1) :59 5 汪复兴.金属物理.北京:机械工业出版社,1981:65 6 Galibois A, Boutenko O. Voyzelle B. Acta Metall, 1980; 28: 1753 7 Schaaber O. Haerterei Tech Mitt, 1967; 22: 1 8 Strunk H, Goesele U. Appl Phys Lett, 1979; 34: 530 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|