| INFLUENCE OF PRE-TRANSFORMED MARTENSITE ON KINETICS OF BAINITIC TRANSFORMATION IN GCr15 STEEL |
| LI Chao;WANG Jianli;LIU Jinfang Harbin Institute of Technology |
|
Cite this article:
LI Chao;WANG Jianli;LIU Jinfang Harbin Institute of Technology. INFLUENCE OF PRE-TRANSFORMED MARTENSITE ON KINETICS OF BAINITIC TRANSFORMATION IN GCr15 STEEL. Acta Metall Sin, 1991, 27(1): 16-19.
|
|
|
Abstract The kinetics of bainitic transformation of GCr15 steel below M_s andthe influence of the pre-transformed martensite formed at different temperatures onit at 240℃ isothermally have been investigated by means of magnetic measurementand dilatometry. The supercooled austenite transforms firstly into martensite and thenlower bainite during isothermal process below M_s. With the decrease of isothermaltemperature and the increase of pre-transformed martensite, the bainitic transforma-tion is accelerated by stress-induction effect, and the incubation period is the shor-test at about 200℃. However, the bainitic transformation becomes rather difficult,if the temperature is continued to decrease and the pre-transformed martensite exce-eds a certain limit. Moreover, it seems in a similar manner of the pre-transformedmartensite increased at different temperatures below M_s to be influenced on the su-bsequent bainitic transformation at 240℃ isothermally.
|
|
Received: 18 January 1991
|
1 李超,汪建利.钢铁,1989;24(5) :45 2 Kar R J, Horn R M Zackay V F. Metall Trans, 1979; 10A: 1711 3 汪建利.哈尔滨工业大学硕士学位论文,1988 4 Vasudevan P. Graham L W. Axon H J. J Iron Steel Inst, London, 1958; 190: 386 5 Entwisle A R. Metall Trans. 1971; 2: 2395 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|