Abstract A study of the dissolution equilibrium of Mg vapour in liquid Fe was carriedout at 1873 K in a two-temperature-zone furnace by use of the vapour pressure method. Theequilibrium constant for the reaction Mg(g)=[Mg] and free energy of solution obtained are:K=a_(Mg) /p_(Mg) =0.0236△G°(wt--%)=58300 J/mol
|
|
Received: 18 June 1990
|
1 Ashton M C, Buhr R K, Magny J-G, Davis K O. Ironmaking Steelmaking, 1975; 2: 111 2 Yamaguchi S, Uemura T, Nashiwa H, Sugita H. Ironmaking Steelmaking, 1977; 4: 276 3 Ackermen D M, Hauesn P R. Steelmaking Proceedings 61, Chicago, AIME, 1978: 452 4 赵风林, Gammal T E, Dahl W. 北京钢铁学院学报, 1983; (3) : 1 5 Johanson R. SCANINJECT Int Conf on Injection Metallurgy, Lulea, Sweden, 1977, Jernkontoret. Vol. 18: 1--25 6 Guichelaar P J, Trojan P K, McCluhan T, Flinn R A. Metall, Trans, 1971; 2: 3305 7 周德壁,北京钢铁学院硕士论文,1985 8 Kubaschewski O, Alcock C B. Metallurgical Thermochemistry, London: Pergamon, 1979: 366 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|