| INTERFACE MORPHOLOGIES AND MICROSTRUCTURES DURING DENDRITE-TO-CELL TRANSITION AT HIGH GROWTH RATE |
| LI Jianguo;MAO Xiemin;FU Hengzhi Northwestern Polytechnical University; Xi'an lecturer;Faculty No.403;Northwestern Polytechnical University; Xi'an 710072 |
|
Cite this article:
LI Jianguo;MAO Xiemin;FU Hengzhi Northwestern Polytechnical University; Xi'an lecturer;Faculty No.403;Northwestern Polytechnical University; Xi'an 710072. INTERFACE MORPHOLOGIES AND MICROSTRUCTURES DURING DENDRITE-TO-CELL TRANSITION AT HIGH GROWTH RATE. Acta Metall Sin, 1990, 26(4): 79-82.
|
|
|
Abstract The interface morphologies and microstructures of the directionally solidifiedNi-5wt-%Cu alloy during the dendrite-to-cell transition at high growth rate have been investi-gated by a newly developed equipment for directional solidification. The results show in thevicinity of dendrite-to-cell transition, the well developed sidebranches become shrivelled withthe increase of growth rate and disappear at the dendrite-to-cell transition, and at the sametime the primary spacing decreases. Moreover, the length of mushy zone decreases greatlyduring the dendrite-to-cell transition. Cells obtained at high growth rate have much in commonwith those at low growth rate, but with much smaller cell spacing.
|
|
Received: 18 April 1990
|
1 Mullins W W, Sekerka R F. J Appl Phys, 1964; 35: 444 2 Coriell S R, Sekerka R F. In: Mehrabian R, Kear B H, Cohen M eds., Rapid Solidification Processing Principles and Technologies Ⅱ, Baton Rouge, LA: Claitor's, 1980: 35 3 Boettinger W J, Shectman D, Schaefer R J, Biancaniello F S. Metall Trans, 1984; 15A: 55 4 姜明,黄建国,江晓平,孙晓峰,葛云龙,胡壮麒.材料科学进展,1989;3:348 5 Clayton D N, Hellawell A. In: Solidification, Processing 1987, London: The Institute of Metals, 1988: 156 6 安阁英,刘立新.金属科学与工艺,1985;4(4) :55! |