| ON STABILIZATION OF THERMOELASTIC MARTENSITE IN A Cu-Zn-Al ALLOY |
| WANG Mingpu;LIU Jinwen Central South University of Technology; Changsha lecturer;Department of Materials Science and Engineering;Central South University of Technology;Changsha 410083 |
|
Cite this article:
WANG Mingpu;LIU Jinwen Central South University of Technology; Changsha lecturer;Department of Materials Science and Engineering;Central South University of Technology;Changsha 410083. ON STABILIZATION OF THERMOELASTIC MARTENSITE IN A Cu-Zn-Al ALLOY. Acta Metall Sin, 1990, 26(3): 66-68.
|
|
|
Abstract The stabilization of the thermoelastic martensite in a rapidly solidi-fied Cu-Zn-Al alloy is believed to be an atomic configuration from ordering todisordering, and the transition of martensite structure from M18R to N9R (b/a=1/3~(1/2)). This is dependent upon the intrinsic decomposition tendency of the marten-site.
|
|
Received: 18 March 1990
|
1 Humbeeck J V, Sen J J, Ngoie M, Delaey L. Scr Metall, 1984; 18: 893 2 Graef M D. Humbeeck J V, Andrade M. Delaey L. Scr Metall, 1985; 16: 729 3 祝向永,唐远永,曹明盛.中南矿冶学院学报,1981;12(3) :1U |
| No Suggested Reading articles found! |
|
|