| MICROSTRUCTURES AND PROPERTIES OF Mn-CONTAINING TiAl ALLOYS |
| CAO Mingzhou;HAN Dong;ZHOU Jing;LI Dong Institute of Metal Research; Academia Sinica; Shenyang Associate professor |
|
Cite this article:
CAO Mingzhou;HAN Dong;ZHOU Jing;LI Dong Institute of Metal Research; Academia Sinica; Shenyang Associate professor. MICROSTRUCTURES AND PROPERTIES OF Mn-CONTAINING TiAl ALLOYS. Acta Metall Sin, 1990, 26(3): 69-73.
|
|
|
Abstract The microstructures of Ti-33wt-%Al-(1.6--4.5) wt-%Mn alloys arecomposed of γ+α_2 phases, but the valume of α_2 phase is a little. Mn alloying de-creases the α and c lattice axes of γ phase and the c/α value is more nearly to one,because the atomic radius of Mn is less than the atomic radius of Ti or Al. Mnalloying promotes the formation of twins in γ phase and increases the ability ofplastic deformation of TiAl alloys at room temperature.
|
|
Received: 18 March 1990
|
1 Lipsitt H A, Shechtman D, Schafrik R E. Metall Trans, 1975; 6A: 1991 2 Kawabata T, Kanai T, Izumi O. Acta Metall, 1985; 33: 1355 3 Greenberg B F, Anisimov V I, Gornostirev Y N, Taluts G G. Scr Metall, 1988; 22: 859 4 Vujic D, Li Z X, Wang S H. Metall Trans. 1988; 19A: 2445 5 Kawabata T, Tadano M, Izumi O. Scr Metall. 1988; 22: 172 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|