JIANG Bailing;LEI Tingquan;LIU Wei;CUI Yuexian Harbin Institute of Technology Department of Metallic Materials and Technology;Harbin Institute of Technology; Harbin 150006. TEM OBSERVATION OF NUCLEATION AND GROWTH OF BORIDES DURING BORONIZATION OF STEEL 20 AND INFLUENCE OF PRIOR DEFORMATION. Acta Metall Sin, 1990, 26(2): 41-45.
|
|
|
Abstract TEM observation in situ on the single-side thinned specimens wasmade of the nucleation and growth of borides during boronization of steel 20 andthe influence of prior room temperature deformation. The results of X-ray diffrac-tion and electron probe microstructure analysis show that only Fe_2B formed inthe surface layer of specimens at the beginning of boronization; the atomic concen-tration of B in the surface layer increased with the increase of deformation mon-otonously; and the segregation of B atoms in the dislocation cells hindered the re-covery and recrystallization of the deformed structure of the matrix and accelara-ted the nucleation and growth of borides in the surface layer.
|
|
Received: 18 February 1990
|
1 孙喜臣,林振湛.金属科学与工艺,1988;(3) :49 2 Kastner B, Przybylowicz K. Crygoruk I. Harterei-Tech Mitt, 1979; 34 (4) : 173 3 Ovrutskii A M, Spiridonova I M. Phys Chem Mater Treat, 1983; 17: 322 4 Berzina I G, Gusev E B. Fiz Met Metalloved, 1984; (5) : 926 5 Polanschuetz W. Scr Metall, 1985; 19: 159 6 Lartigue S, Priester L. Acta Metall, 1983; 29: 1809 7 Pond K C, Aronson H I. Scr Metall, 1974; 8: 559 8 Lei T C, Liu H J, Liu Z R. In: Lei T C, Igata N eds., Proc the University of Tokyo-Harbin Institute of Technology Symposium on Material Science, Tokyo: University of Tokyo, 1985: |