PRECIPITATION IN BINARY Al-Li ALLOYS
YAO Daping;HU Zhuangqi;ZHANG Yun;SHI Changxu Institute of Metal Research; Academia Sinica; Shenyang Institute of Metal Research;Academia Sinica;Shenyang 110015
Cite this article: 

YAO Daping;HU Zhuangqi;ZHANG Yun;SHI Changxu Institute of Metal Research; Academia Sinica; Shenyang Institute of Metal Research;Academia Sinica;Shenyang 110015. PRECIPITATION IN BINARY Al-Li ALLOYS. Acta Metall Sin, 1990, 26(2): 46-51.

Download:  PDF(1066KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Studies were carried out of the precipitation in two sets of binaryAl-Li alloys by means of hardness test, DSC analysis and TEM observation. Whent healloys were aged for constant time, a peak appeared on the plot of temperaturedependence upon their hardness in the range of low temperature, and the endother-mic dissolution peak was quite distinct on the DSC curve also at low temperature.These are believed that an li-rich GP zone is formed in the alloys aged at lowtemperature, but no more GP zone if aging at elevated temperature. The hardnessof the alloys raises rapidly with coarsening of δ'-phase grains. The two endother-mic peaks of δ' dissolution on the DSC curve are related to the structural adjust-ment at twice of the δ' precipitation. The equilibrium δ-phase, being of higherthermal stability, nucleates and grows directly from the supersaturated solidsolution with the aid of the grain boundary.
Key words:  binary Al-Li alloy      precipitation      dissolution      endothermic peak      aging     
Received:  18 February 1990     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1990/V26/I2/46

1 Silcock J M. J Inst Met, 1959--60; 88: 357
2 Nozato R, Nakai G. Trans Jpn Inst Met, 1977; 18: 679
3 Papazian J M, Sigli C, Sanchez J M. Scr Metall. 1986; 20: 201
4 Balmuth E S. Scr Metall, 1984; 18: 301
5 Mukhopadhyay A K, Tite C N J, Flower H M, Gregson P J, Sale F. In: Champier G. Dubost B, Miannay D, Sabetay L eds., Aluminum-Lithium Alloys IV, J Phys (Paris) Colloque, 1987; 3: C3--439
6 Yao Daping, Hu Zhuangqi, Li Yiyi, Zhang Yun, Shi Changxu. Chin J Me. Sci Technol, to be published
7 Baumann S F, Williams D B. Acta Metall, 1985; 33: 1069
8 高桥恒夫,里逹雄,轻金属,1986;36(4) ;207
9 Yao D P, Zhang Y, Hu Z Q, Li Y Y, Shi C X. Scr Metall, 1989; 23: 537Z
[1] ZHANG Leilei, CHEN Jingyang, TANG Xin, XIAO Chengbo, ZHANG Mingjun, YANG Qing. Evolution of Microstructures and Mechanical Properties of K439B Superalloy During Long-Term Aging at 800oC[J]. 金属学报, 2023, 59(9): 1253-1264.
[2] LIANG Kai, YAO Zhihao, XIE Xishan, YAO Kaijun, DONG Jianxin. Correlation Between Microstructure and Properties of New Heat-Resistant Alloy SP2215[J]. 金属学报, 2023, 59(6): 797-811.
[3] WANG Changsheng, FU Huadong, ZHANG Hongtao, XIE Jianxin. Effect of Cold-Rolling Deformation on Microstructure, Properties, and Precipitation Behavior of High-Performance Cu-Ni-Si Alloys[J]. 金属学报, 2023, 59(5): 585-598.
[4] WANG Bin, NIU Mengchao, WANG Wei, JIANG Tao, LUAN Junhua, YANG Ke. Microstructure and Strength-Toughness of a Cu-Contained Maraging Stainless Steel[J]. 金属学报, 2023, 59(5): 636-646.
[5] LIU Manping, XUE Zhoulei, PENG Zhen, CHEN Yulin, DING Lipeng, JIA Zhihong. Effect of Post-Aging on Microstructure and Mechanical Properties of an Ultrafine-Grained 6061 Aluminum Alloy[J]. 金属学报, 2023, 59(5): 657-667.
[6] ZHU Yunpeng, QIN Jiayu, WANG Jinhui, MA Hongbin, JIN Peipeng, LI Peijie. Microstructure and Properties of AZ61 Ultra-Fine Grained Magnesium Alloy Prepared by Mechanical Milling and Powder Metallurgy Processing[J]. 金属学报, 2023, 59(2): 257-266.
[7] MA Guonan, ZHU Shize, WANG Dong, XIAO Bolv, MA Zongyi. Aging Behaviors and Mechanical Properties of SiC/Al-Zn-Mg-Cu Composites[J]. 金属学报, 2023, 59(12): 1655-1664.
[8] GONG Xiangpeng, WU Cuilan, LUO Shifang, SHEN Ruohan, YAN Jun. Effect of Natural Aging on Artificial Aging of an Al-2.95Cu-1.55Li-0.57Mg-0.18Zr Alloy at 160oC[J]. 金属学报, 2023, 59(11): 1428-1438.
[9] GENG Yaoxiang, TANG Hao, XU Junhua, ZHANG Zhijie, YU Lihua, JU Hongbo, JIANG Le, JIAN Jianglin. Formability and Mechanical Properties of High-Strength Al-(Mn, Mg)-(Sc, Zr) Alloy Produced by Selective Laser Melting[J]. 金属学报, 2022, 58(8): 1044-1054.
[10] REN Ping, CHEN Xingpin, WANG Cunyu, YU Feng, CAO Wenquan. Effects of Pre-Strain and Two-Step Aging on Microstructure and Mechanical Properties of Fe-30Mn-11Al-1.2C Austenitic Low-Density Steel[J]. 金属学报, 2022, 58(6): 771-780.
[11] GAO Chuan, DENG Yunlai, WANG Fengquan, GUO Xiaobin. Effect of Creep Aging on Mechanical Properties of Under-Aged 7075 Aluminum Alloy[J]. 金属学报, 2022, 58(6): 746-759.
[12] TANG Shuai, LAN Huifang, DUAN Lei, JIN Jianfeng, LI Jianping, LIU Zhenyu, WANG Guodong. Co-Precipitation Behavior in Ferrite Region During Isothermal Process in Ti-Mo-Cu Microalloyed Steel[J]. 金属学报, 2022, 58(3): 355-364.
[13] YUAN Bo, GUO Mingxing, HAN Shaojie, ZHANG Jishan, ZHUANG Linzhong. Effect of 3%Zn Addition on the Non-Isothermal Precipitation Behaviors of Al-Mg-Si-Cu Alloys[J]. 金属学报, 2022, 58(3): 345-354.
[14] HAN Ruyang, YANG Gengwei, SUN Xinjun, ZHAO Gang, LIANG Xiaokai, ZHU Xiaoxiang. Austenite Grain Growth Behavior of Vanadium Microalloying Medium Manganese Martensitic Wear-Resistant Steel[J]. 金属学报, 2022, 58(12): 1589-1599.
[15] SUN Shijie, TIAN Yanzhong, ZHANG Zhefeng. Strengthening and Toughening Mechanisms of Precipitation- Hardened Fe53Mn15Ni15Cr10Al4Ti2C1 High-Entropy Alloy[J]. 金属学报, 2022, 58(1): 54-66.
No Suggested Reading articles found!