INFLUENCE OF GRAIN SIZE AND ORDERING DEGREE OF PARENT PHASE ON M_s IN A Cu-Zn-Al ALLOY CONTAINING B
WU Jianxin;JIANG Bohong;XU Zuyao T. Y. Hsu Shanghai Jiaotong University
Cite this article: 

WU Jianxin;JIANG Bohong;XU Zuyao T. Y. Hsu Shanghai Jiaotong University. INFLUENCE OF GRAIN SIZE AND ORDERING DEGREE OF PARENT PHASE ON M_s IN A Cu-Zn-Al ALLOY CONTAINING B. Acta Metall Sin, 1989, 25(2): 22-28.

Download:  PDF(561KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Based on the thermodynamics of phase transformation, a linear relation-ship between the starting temperature of martensitic transformation and the recipro-cal of the squareroot of grain size has been obtained, i. e. M_s temperature decreaseswith the increasing grain size. It shows a good agreement with the results of elec-tric resistance measurements. Application of Landau's theory gives a quantitative re-lationship between M_s temperature and the ordering parameter of the parent phase,which is well confirmed by the results of X-ray diffraction and electric resistancemeasurements. The activation energy of the DO_3 ordering process in the parent phaseof the alloy is calculated to be 46 kJ/mol.
Key words:  Cu-ZD--Al alloy      shape memory alloy      thermoelastic martensite      grain size      ordering degree     
Received:  18 February 1989     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1989/V25/I2/22

1 Melton K N, Mercier O. In: Haasen P, Gerold V, Kostorz G eds., Strength of Metals and Alloys, Vol. Ⅱ, Pergamon Press, 1979: 1243
2 Enami K, Takimoto N, Nenno S. J Phys (Paris), 1982; 43 (12) : C4--673
3 Ikai Y. J Phys (Paris), 1982; 43 (12) : C4--773
4 Adnyana Dewa N. Metallography, 1985; 18: 187
5 #12
6 唯木次男.日本金属学会会报,1982;21:170
7 Qi Xuan, Jiang Bohong, Hsu T Y (Xu Zuyao), In: Chu Youyi, Hsu T Y, Ko T eds., Shape Memory Alloy's 86, Proc of the Int Symp. on Shape Memory Alloy, Sept. 6--9, 1986, Guilin. China, China Academic Publ., 1986
8 Tong H C, Wayman C M. Acta Metall, 1975; 23: 209
9 Landau L D, Lifshitz C M. In: Sykes J B, Kearsley M J. Statistical Physics, Part 1, 3rd Edition, Pergamon Press, 1980
10 Clark J S, Brown N. J Phys Chem Solids, 1961; 19: 291
11 Cook J M, Brown L M. Scr Metall. 1978; 12: 948_
[1] LI Fulin, FU Rui, BAI Yunrui, MENG Lingchao, TAN Haibing, ZHONG Yan, TIAN Wei, DU Jinhui, TIAN Zhiling. Effects of Initial Grain Size and Strengthening Phase on Thermal Deformation and Recrystallization Behavior of GH4096 Superalloy[J]. 金属学报, 2023, 59(7): 855-870.
[2] CHEN Fei, QIU Pengcheng, LIU Yang, SUN Bingbing, ZHAO Haisheng, SHEN Qiang. Microstructure and Mechanical Properties of NiTi Shape Memory Alloys by In Situ Laser Directed Energy Deposition[J]. 金属学报, 2023, 59(1): 180-190.
[3] YANG Chao, LU Haizhou, MA Hongwei, CAI Weisi. Research and Development in NiTi Shape Memory Alloys Fabricated by Selective Laser Melting[J]. 金属学报, 2023, 59(1): 55-74.
[4] ZHANG Xin, CUI Bo, SUN Bin, ZHAO Xu, ZHANG Xin, LIU Qingsuo, DONG Zhizhong. Effect of Y Element on the Properties of Cu-Al-Ni High Temperature Shape Memory Alloy[J]. 金属学报, 2022, 58(8): 1065-1071.
[5] YUAN Jiahua, ZHANG Qiuhong, WANG Jinliang, WANG Lingyu, WANG Chenchong, XU Wei. Synergistic Effect of Magnetic Field and Grain Size on Martensite Nucleation and Variant Selection[J]. 金属学报, 2022, 58(12): 1570-1580.
[6] JIANG Jiang, HAO Shijie, JIANG Daqiang, GUO Fangmin, REN Yang, CUI Lishan. Lüders-Like Deformation and Stress Transfer Behavior in an In Situ NiTi-NbTi Composite[J]. 金属学报, 2021, 57(7): 921-927.
[7] YE Junjie, HE Zhirong, ZHANG Kungang, DU Yuqing. Effect of Ageing on Microsturcture, Tensile Properties, and Shape Memory Behaviors of Ti-50.8Ni-0.1Zr Shape Memory Alloy[J]. 金属学报, 2021, 57(6): 717-724.
[8] ZUO Liang, LI Zongbin, YAN Haile, YANG Bo, ZHAO Xiang. Texturation and Functional Behaviors of Polycrystalline Ni-Mn-X Phase Transformation Alloys[J]. 金属学报, 2021, 57(11): 1396-1415.
[9] XIAO Fei, CHEN Hong, JIN Xuejun. Research Progress in Elastocaloric Cooling Effect Basing on Shape Memory Alloy[J]. 金属学报, 2021, 57(1): 29-41.
[10] ZHANG Shouqing, HU Xiaofeng, DU Yubin, JIANG Haichang, PANG Huiyong, RONG Lijian. Cross-Section Effect of Ni-Cr-Mo-B Ultra-Heavy Steel Plate for Offshore Platform[J]. 金属学报, 2020, 56(9): 1227-1238.
[11] XU Zhanyi, SHA Yuhui, ZHANG Fang, ZHANG Huabing, LI Guobao, CHU Shuangjie, ZUO Liang. Orientation Selection Behavior During Secondary Recrystallization in Grain-Oriented Silicon Steel[J]. 金属学报, 2020, 56(8): 1067-1074.
[12] HE Shuwen, WANG Minghua, BAI Qin, XIA Shuang, ZHOU Bangxin. Effect of TaC Content on Microstructure and Mechanical Properties of WC-TiC-TaC-Co Cemented Carbide[J]. 金属学报, 2020, 56(7): 1015-1024.
[13] CHEN Xiang,CHEN Wei,ZHAO Yang,LU Sheng,JIN Xiaoqing,PENG Xianghe. Assembly Performance Simulation of NiTiNb Shape Memory Alloy Pipe Joint Considering Coupling Effect of Phase Transformation and Plastic Deformation[J]. 金属学报, 2020, 56(3): 361-373.
[14] HUA Hanyu,XIE Jun,SHU Delong,HOU Guichen,Naicheng SHENG,YU Jinjiang,CUI Chuanyong,SUN Xiaofeng,ZHOU Yizhou. Influence of W Content on the Microstructure of Nickel Base Superalloy with High W Content[J]. 金属学报, 2020, 56(2): 161-170.
[15] Xin LI,Yuecheng DONG,Zhenhua DAN,Hui CHANG,Zhigang FANG,Yanhua GUO. Corrosion Behavior of Ultrafine Grained Pure Ti Processed by Equal Channel Angular Pressing[J]. 金属学报, 2019, 55(8): 967-975.
No Suggested Reading articles found!