| ELECTRONIC STRUCTURE OF Cu DOPED RECo_5 TYPE INTERMETALLIC COMPOUNDS |
| LIU Senying;GAO Zhe;LI Keng;LI Junqing;WANG Congyu University of Science and Technology Beijing China University of Science and Technology Beijing Central Iron and Steel Research Institute |
|
Cite this article:
LIU Senying;GAO Zhe;LI Keng;LI Junqing;WANG Congyu University of Science and Technology Beijing China University of Science and Technology Beijing Central Iron and Steel Research Institute. ELECTRONIC STRUCTURE OF Cu DOPED RECo_5 TYPE INTERMETALLIC COMPOUNDS. Acta Metall Sin, 1989, 25(2): 15-21.
|
|
|
Abstract Based on the feature of crystal sites occupied by alloying elements, amodel cluster, investigating the interaction mechanisms of nonmagnetic element Cuin RECo_5 type alloy, has been presented. The electronic structure has been calcula-ted with SCF-X_α-SW method. The calculating results show that, after Cu replaced2c crystal site Co, the energy spectrum of the model cluster will move towards shal-low trap potential, energy gap will become small, the charge among the atoms willredistribute, and some new states to which impurity contributes will produce. Partial-wave local density of states gives the interactions between atoms. Results of Hellm-man-Feynman force show that thermal expansion anisotropy of the model clusterdecreases considerably after Cu substitutes for 2c crystal site Co.
|
|
Received: 18 February 1989
|
1 杨应昌,何文望,林勤.金属学报,1981;17:67 2 孙天铎,祝景汉,王德文.金属学报,1979;15:58 3 Slater J C, Johnson K H. Phys Rev, 1972; B5: 844 4 Johnson K H, Smith F C Jr. Phys Rev, 1972; B5: 831 5 Norman J G Jr. J Chem Phys, 1974; 61: 4630 6 Case D A, Karplus M. Chem Phys Lett, 1976; 39; 33 7 Case D A, Karplus M. J Am Chem Soc, 1977; 99: 6182f |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |