Please wait a minute...
Acta Metall Sin  1988, Vol. 24 Issue (6): 505-510    DOI:
Current Issue | Archive | Adv Search |
STUDY OF HYDROGEN DISTRIBUTION AND DIFFUSION BEHAVIOUR IN HIGH PRESSURE HYDROGEN CHARGED AUSTENITIC STEEL BY IMMA
MA Luming;LI Yiyi;LIU Shuwang;CHEN Lian Institute of Metal Research; Academia Sinica; Shenyang
Cite this article: 

MA Luming;LI Yiyi;LIU Shuwang;CHEN Lian Institute of Metal Research; Academia Sinica; Shenyang. STUDY OF HYDROGEN DISTRIBUTION AND DIFFUSION BEHAVIOUR IN HIGH PRESSURE HYDROGEN CHARGED AUSTENITIC STEEL BY IMMA. Acta Metall Sin, 1988, 24(6): 505-510.

Download:  PDF(446KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The hydrogen distribution curve along cross-section of austenitic steel21Cr-7Ni-9Mn-N was obtained quantitatively by IMMA (Ion Microprobe MassAnalyzer) with high pressure hydrogen charging specimen. Thus, the hydrogen sol-ubility and diffusivity may be measured as well as the hydrogen permeability andother parameters may be calculated indirectly. The hydrogen distribution in speci-mens either long-term aged in air or electron beam weld seam after high pressurehydrogen charged was also examined.
Key words:  High pressure hydrogen charging      ion microprobe analysis      austenitic steel      diffusion     
Received:  18 June 1988     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1988/V24/I6/505

1 Magee C W, Botnick E M. J Vac Sci Technol, 1981; 19: 47
2 吕曼祺,刘宝昌,范存淦,李依依.中国科学院金属研究所内部资料,(待发表)
3 孙秀魁,徐坚.中国腐蚀与防护学报,1987;7:274
4 Quick N R, Johnson H H. Metall Trans, 1979; 10A: 67
5 Nelson H G, Stein J E. NASA Rep. TND-7265, 1972
6 Kass W J, Axdrzejewski W J. AEC Rep. Sc-DR-72-0136, 1972
7 Louthan M R, Derrick R G. Corros Sei, 1975; 15: 565
8 Tanabe T, Yamanishi Y, Sawada K. Imoto S. J Nucl Mater, 1984; 122--123: 1568
9 Chen Lian (陈廉), Zou Junjun (邹军军). Proc 2nd Beijing Conf and Exhib on Instrum Analysis, 1987: 369
[1] GONG Shengkai, LIU Yuan, GENG Lilun, RU Yi, ZHAO Wenyue, PEI Yanling, LI Shusuo. Advances in the Regulation and Interfacial Behavior of Coatings/Superalloys[J]. 金属学报, 2023, 59(9): 1097-1108.
[2] XU Wenguo, HAO Wenjiang, LI Yingju, ZHAO Qingbin, LU Bingyu, GUO Heyi, LIU Tianyu, FENG Xiaohui, YANG Yuansheng. Effects of Trace Aluminum and Titanium on High Temper-ature Oxidation Behavior of Inconel 690 Alloy[J]. 金属学报, 2023, 59(12): 1547-1558.
[3] LIU Lujun, LIU Zheng, LIU Renhui, LIU Yong. Grain Boundary Structure and Coercivity Enhancement of Nd90Al10 Alloy Modified NdFeB Permanent Magnets by GBD Process[J]. 金属学报, 2023, 59(11): 1457-1465.
[4] LI Sai, YANG Zenan, ZHANG Chi, YANG Zhigang. Phase Field Study of the Diffusional Paths in Pearlite-Austenite Transformation[J]. 金属学报, 2023, 59(10): 1376-1388.
[5] SHEN Yingying, ZHANG Guoxing, JIA Qing, WANG Yumin, CUI Yuyou, YANG Rui. Interfacial Reaction and Thermal Stability of the SiCf/TiAl Composites[J]. 金属学报, 2022, 58(9): 1150-1158.
[6] LI Xifeng, LI Tianle, AN Dayong, WU Huiping, CHEN Jieshi, CHEN Jun. Research Progress of Titanium Alloys and Their Diffusion Bonding Fatigue Characteristics[J]. 金属学报, 2022, 58(4): 473-485.
[7] HUA Yu, CHEN Jianguo, YU Liming, SI Yonghong, LIU Chenxi, LI Huijun, LIU Yongchang. Microstructure Evolution and Mechanical Properties of Dissimilar Material Diffusion-Bonded Joint for High Cr Ferrite Heat-Resistant Steel and Austenitic Heat-Resistant Steel[J]. 金属学报, 2022, 58(2): 141-154.
[8] LIU Zhongwu, HE Jiayi. Several Issues on the Development of Grain Boundary Diffusion Process for Nd-Fe-B Permanent Magnets[J]. 金属学报, 2021, 57(9): 1155-1170.
[9] CHEN Shenghu, RONG Lijian. Oxide Scale Formation on Ultrafine-Grained Ferritic-Martensitic Steel During Pre-Oxidation and Its Effect on the Corrosion Performance in Stagnant Liquid Pb-Bi Eutectic[J]. 金属学报, 2021, 57(8): 989-999.
[10] LI Juan, ZHAO Honglong, ZHOU Nian, ZHANG Yingzhe, QIN Qingdong, SU Xiangdong. Diffusion Bonding of CoCrFeNiCu High-Entropy Alloy to 304 Stainless Steel[J]. 金属学报, 2021, 57(12): 1567-1578.
[11] LIU Chenxi, MAO Chunliang, CUI Lei, ZHOU Xiaosheng, YU Liming, LIU Yongchang. Recent Progress in Microstructural Control and Solid-State Welding of Reduced Activation Ferritic/Martensitic Steels[J]. 金属学报, 2021, 57(11): 1521-1538.
[12] SUN Zhengyang, YANG Chao, LIU Wenbo. Phase Field Simulations of the Sintering Process of UO2[J]. 金属学报, 2020, 56(9): 1295-1303.
[13] WANG Chao, ZHANG Xu, WANG Yumin, YANG Qing, YANG Lina, ZHANG Guoxing, WU Ying, KONG Xu, YANG Rui. Mechanisms of Interfacial Reaction and Matrix Phase Transition in SiCf /Ti65 Composites[J]. 金属学报, 2020, 56(9): 1275-1285.
[14] DING Wen, WANG Xiaojing, LIU Ning, QIN Liang. Diffusion Bonding of Copper and 304 Stainless Steel with an Interlayer of CoCrFeMnNi High-Entropy Alloy[J]. 金属学报, 2020, 56(8): 1084-1090.
[15] SUN Zhengyang, WANG Yutian, LIU Wenbo. Phase-Field Simulation of the Interaction Between Pore and Grain Boundary[J]. 金属学报, 2020, 56(12): 1643-1653.
No Suggested Reading articles found!