LOCALIZED CORROSION OF MICROCRYSTALS OF 1Cr18Ni9Ti STAINLESS STEEL
LIU Dacheng;CAO Chunan;WANG Fuhui;LOU Hanyi;ZHANG Lixin Institute of Corrosion and Protection of Metals; Academia Sinica; Shenyang
Cite this article: 

LIU Dacheng;CAO Chunan;WANG Fuhui;LOU Hanyi;ZHANG Lixin Institute of Corrosion and Protection of Metals; Academia Sinica; Shenyang. LOCALIZED CORROSION OF MICROCRYSTALS OF 1Cr18Ni9Ti STAINLESS STEEL. Acta Metall Sin, 1988, 24(5): 441-443.

Download:  PDF(248KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The resistance against localized corrosion of 1Cr18Ni9Ti microcrystals with nor-mal grain size and bcc structure obtained by magnetron sputtering has been compared. Two kindsof microcrystals with (110) and (211) textures respectively were obtained under different sputter-ing conditions. Both microcrystals were found to have better resistance against localized corrosionthan the crystal with normal grain. The microcrystal with (110) perferred orientation has largerresistance to localized carrosion than that with (211)preferred orientation
Key words:  microcrystal      localized corrosion      magnetron sputtering     
Received:  18 May 1988     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1988/V24/I5/441

1 张云汉,刘立民.中国真空学会薄膜专业委员会全国第一届PVD学术讨论会论文摘要,1986:65
2 Nowak W B. Mater Sci Eng, 1976; 23: 301
3 Bertocci U, Kruger J. Surf Sci, 1980; 101: 608
4 曹楚南,常晓元,林海潮.中国腐蚀与防护学报,(待发表)
[1] HUANG Ding, QIAO Yanxin, YANG Lanlan, WANG Jinlong, CHEN Minghui, ZHU Shenglong, WANG Fuhui. Effect of Shot Peening of Substrate Surface on Cyclic Oxidation Behavior of Sputtered Nanocrystalline Coating[J]. 金属学报, 2023, 59(5): 668-678.
[2] HU Wenbin, ZHANG Xiaowen, SONG Longfei, LIAO Bokai, WAN Shan, KANG Lei, GUO Xingpeng. Corrosion Behavior of AlCoCrFeNi2.1 Eutectic High-Entropy Alloy in Sulfuric Acid Solution[J]. 金属学报, 2023, 59(12): 1644-1654.
[3] XIA Dahai, DENG Chengman, CHEN Ziguang, LI Tianshu, HU Wenbin. Modeling Localized Corrosion Propagation of Metallic Materials by Peridynamics: Progresses and Challenges[J]. 金属学报, 2022, 58(9): 1093-1107.
[4] CAO Qingping, LV Linbo, WANG Xiaodong, JIANG Jianzhong. Magnetron Sputtering Metal Glass Film Preparation and the “Specimen Size Effect” of the Mechanical Property[J]. 金属学报, 2021, 57(4): 473-490.
[5] LIU Yanmei, WANG Tiegang, GUO Yuyao, KE Peiling, MENG Deqiang, ZHANG Jifu. Design, Preparation and Properties of Ti-B-N Nanocomposite Coatings[J]. 金属学报, 2020, 56(11): 1521-1529.
[6] Wentao LI,Zhenyu WANG,Dong ZHANG,Jianguo PAN,Peiling KE,Aiying WANG. Preparation of Ti2AlC Coating by the Combination of a Hybrid Cathode Arc/Magnetron Sputtering with Post-Annealing[J]. 金属学报, 2019, 55(5): 647-656.
[7] Shasha YANG,Feng YANG,Minghui CHEN,Yunsong NIU,Shenglong ZHU,Fuhui WANG. Effect of Nitrogen Doping on Microstructure and Wear Resistance of Tantalum Coatings Deposited by Direct Current Magnetron Sputtering[J]. 金属学报, 2019, 55(3): 308-316.
[8] Houpu WU,Xiubo TIAN,Xinyu ZHANG,Chunzhi GONG. Discharge Characteristics of Novel Dual-Pulse HiPIMS and Deposition of CrN Films with High Deposition Rate[J]. 金属学报, 2019, 55(3): 299-307.
[9] Huiying SHI, Chao YANG, Bailing JIANG, Bei HUANG, Di WANG. Influences of Target Peak Current Density on the Microstructure and Mechanical Properties of TiN Films Deposited by Dual Pulsed Power Magnetron Sputtering[J]. 金属学报, 2018, 54(6): 927-934.
[10] Baiyang LOU,Yuxing WANG. EFFECTS OF Mo CONTENT ON THE MICRO-STRUCTURE AND TRIBOLOGICAL PROPERTIES OF CrMoAlN FILMS[J]. 金属学报, 2016, 52(6): 727-733.
[11] Xudong SUI,Guojian LI,Qiang WANG,Xuesi QIN,Xiangkui ZHOU,Kai WANG,Lijian ZUO. PREPARATION OF Ti1-xAlxN COATING IN CUTTING TITANIUM ALLOY AND ITS CUTTING PERFORMANCE[J]. 金属学报, 2016, 52(6): 741-746.
[12] QI Dongli, LEI Hao, FAN Di, PEI Zhiliang, GONG Jun, SUN Chao. EFFECT OF Mo CONTENT ON THE MICROSTRUC-TURE AND PROPERTIES OF CrMoN COMPOSITE COATINGS[J]. 金属学报, 2015, 51(3): 371-377.
[13] ZHONG Xiaocong, JIANG Liangxing, LÜ Xiaojun, LAI Yanqing, LI Jie, LIU Yexiang. EFFECTS OF CHLORIDE ION ON THE ELECTRO- CHEMICAL BEHAVIOR OF Pb-Ag-RE ALLOY ANODE[J]. 金属学报, 2015, 51(3): 378-384.
[14] Chao YANG,Bailing JIANG,Lin FENG,Juan HAO. EFFECT OF DISCHARGE CHARACTERISTICS OF TARGET ON IONIZATION AND DEPOSITION OF DEPOSITED PARTICLES[J]. 金属学报, 2015, 51(12): 1523-1530.
[15] Wenfang CUI,Dong CAO,Gaowu QIN. MICROSTRUCTURE AND WEAR RESISTANCE OF Ti/TiN MULTILAYER FILMS DEPOSITED BY MAGNETRON SPUTTERING[J]. 金属学报, 2015, 51(12): 1531-1537.
No Suggested Reading articles found!