EFFECT OF AUSTENITE STRENGTHENING ON MARTENSITIC AND BAINITIC TRANSFORMATIONS
XU Zuyao (T.Y. Hsu);CHEN Weizhong Shanghai Jiaotong UniversityDepartment of Materials Science;Shanghai Jiaotong University
Cite this article: 

XU Zuyao (T.Y. Hsu);CHEN Weizhong Shanghai Jiaotong UniversityDepartment of Materials Science;Shanghai Jiaotong University. EFFECT OF AUSTENITE STRENGTHENING ON MARTENSITIC AND BAINITIC TRANSFORMATIONS. Acta Metall Sin, 1988, 24(3): 155-160.

Download:  PDF(418KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Effect of austenite strengthening on M_s and B_s temperatures in Fe-Ni-C alloys and some commercial steels have been studied. M_s temperature lowers1inearly with the increase of the yield strength of the austenite, while B_s seems tobe independent of the austenite strengthening. By plotting B_s temperature of thethree Fe-Ni-C alloys versus D~γ(C) and D~γ(Fe), a linear relation is obtained. The△G_v and D~γ(Fe) of the alloys were calculated at the nose temperatures in TTT di-agrams, and the incubation periods are found to be directly proportional to thevalues deduced from Feder's equation for diffusional transformations, implying thatthe incubation period at the nose temperature of bainitic transformation is gov-erned by the change in free energy and the diffusion of iron atoms in austenite.
Key words:  Austenite strengthening      martensite      bainite      transformations     
Received:  18 March 1988     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1988/V24/I3/155

1 Hsu T Y(Xu Zuyao), Li Jian, Zen Zhengpeng. Metallography, 1986; 19: 305
2 徐祖耀,李箭,曾振鹏.金属学报,1986;22:A494
3 Ansell G S, Brofman P J, Nichol T J, Judd G. ICOMAT-79, Cambridge, Massachusetts, 1979: 350
4 Breinan B M, Ansell G S. Metall Trans, 1970; 1: 1513
5 Hsu T Y(Xu Zuyao). J Mater Sci, 1985; 20: 23
6 Chang Hongbing, Hsu T Y (Xu Zuyao). Acta Metall, 1986; 34: 325
7 Hsu T Y (Xu Zuyao), Mou Yiwen. Acta Metall, 1984; 32: 1469
8 Wells C, Mehl R F. Trans AIME, 1940; 140: 279
9 #12
10 Feder J, Russell K C, Lothe J, Pound G M. Adv Phys, 1966; 15: 111
11 徐祖耀.马氏体相变与马氏体,北京:科学出版社,1980:90--91
12 Romig A D Jr, Goldstein J I. Metall Trans A, 1980; 11(7) : 1151
[1] WANG Zhoutou, YUAN Qing, ZHANG Qingxiao, LIU Sheng, XU Guang. Microstructure and Mechanical Properties of a Cold Rolled Gradient Medium-Carbon Martensitic Steel[J]. 金属学报, 2023, 59(6): 821-828.
[2] ZHAO Yafeng, LIU Sujie, CHEN Yun, MA Hui, MA Guangcai, GUO Yi. Critical Inclusion Size and Void Growth in Dual-Phase Ferrite-Bainite Steel During Ductile Fracture[J]. 金属学报, 2023, 59(5): 611-622.
[3] CHEN Xueshuang, HUANG Xingmin, LIU Junjie, LV Chao, ZHANG Juan. Microstructure Regulation and Strengthening Mechanisms of a Hot-Rolled & Intercritical Annealed Medium-Mn Steel Containing Mn-Segregation Band[J]. 金属学报, 2023, 59(11): 1448-1456.
[4] HOU Xuru, ZHAO Lin, REN Shubin, PENG Yun, MA Chengyong, TIAN Zhiling. Effect of Heat Input on Microstructure and Mechanical Properties of Marine High Strength Steel Fabricated by Wire Arc Additive Manufacturing[J]. 金属学报, 2023, 59(10): 1311-1323.
[5] LI Xiaolin, LIU Linxi, LI Yating, YANG Jiawei, DENG Xiangtao, WANG Haifeng. Mechanical Properties and Creep Behavior of MX-Type Precipitates Strengthened Heat Resistant Martensite Steel[J]. 金属学报, 2022, 58(9): 1199-1207.
[6] ZHU Bin, YANG Lan, LIU Yong, ZHANG Yisheng. Micromechanical Properties of Duplex Microstructure of Martensite/Bainite in Hot Stamping via the Reverse Algorithms in Instrumented Sharp Indentation[J]. 金属学报, 2022, 58(2): 155-164.
[7] ZHENG Chun, LIU Jiabin, JIANG Laizhu, YANG Cheng, JIANG Meixue. Effect of Tensile Deformation on Microstructure and Corrosion Resistance of High Nitrogen Austenitic Stainless Steels[J]. 金属学报, 2022, 58(2): 193-205.
[8] ZHU Dongming, HE Jiangli, SHI Genhao, WANG Qingfeng. Effect of Welding Heat Input on Microstructure and Impact Toughness of the Simulated CGHAZ in Q500qE Steel[J]. 金属学报, 2022, 58(12): 1581-1588.
[9] JIANG Zhonghua, DU Junyi, WANG Pei, ZHENG Jianneng, LI Dianzhong, LI Yiyi. Mechanism of Improving the Impact Toughness of SA508-3 Steel Used for Nuclear Power by Pre-Transformation of M-A Islands[J]. 金属学报, 2021, 57(7): 891-902.
[10] SHI Zengmin, LIANG Jingyu, LI Jian, WANG Maoqiu, FANG Zifan. In Situ Analysis of Plastic Deformation of Lath Martensite During Tensile Process[J]. 金属学报, 2021, 57(5): 595-604.
[11] WANG Yu, HU Bin, LIU Xingyi, ZHANG Hao, ZHANG Haoyun, GUAN Zhiqiang, LUO Haiwen. Influence of Annealing Temperature on Both Mechanical and Damping Properties of Nb-Alloyed High Mn Steel[J]. 金属学报, 2021, 57(12): 1588-1594.
[12] LUO Haiwen,SHEN Guohui. Progress and Perspective of Ultra-High Strength Steels Having High Toughness[J]. 金属学报, 2020, 56(4): 494-512.
[13] WANG Shihong,LI Jian,GE Xin,CHAI Feng,LUO Xiaobing,YANG Caifu,SU Hang. Microstructural Evolution and Work Hardening Behavior of Fe-19Mn Alloy Containing Duplex Austenite and ε-Martensite[J]. 金属学报, 2020, 56(3): 311-320.
[14] ZHU Jian, ZHANG Zhihao, XIE Jianxin. Plastic Deformation Behavior and Fracture Mechanism of Rare Earth H13 Steel Based on In Situ TEM Tensile Study[J]. 金属学报, 2020, 56(12): 1592-1604.
[15] Miao JIN, Wenquan LI, Shuo HAO, Ruixue MEI, Na LI, Lei CHEN. Effect of Solution Temperature on Tensile Deformation Behavior of Mn-N Bearing Duplex Stainless Steel[J]. 金属学报, 2019, 55(4): 436-444.
No Suggested Reading articles found!