Please wait a minute...
Acta Metall Sin  1988, Vol. 24 Issue (1): 63-65    DOI:
Current Issue | Archive | Adv Search |
IMPROVEMENT OF HIGH TEMPERATURE WEAR RESISTANCE BY INJECTION OF OXIDE PARTICLES FOR Fe-BASE ALLOYS
ZHANG Yun;ZHAO Hong'en;GUO Jianting Institute of Metal Research; Academia Sinica; Shenyang
Cite this article: 

ZHANG Yun;ZHAO Hong'en;GUO Jianting Institute of Metal Research; Academia Sinica; Shenyang. IMPROVEMENT OF HIGH TEMPERATURE WEAR RESISTANCE BY INJECTION OF OXIDE PARTICLES FOR Fe-BASE ALLOYS. Acta Metall Sin, 1988, 24(1): 63-65.

Download:  PDF(633KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The microstructure and mechanical properties of 1Cr18Ni9Ti, FeCrAl andCr25Ni20SiMn alloys after injection of oxide particles have been determined. The results showthat the tensile strength and hardness at room temperature or high temperatures, the high temper-ature rupture strength as well as the oxidation-wear resistance at high temperatures of the alloysincrease owing to the injection.
Key words:  high temperature wear resistance      Fe-base alloys      oxide      injection     
Received:  18 January 1988     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1988/V24/I1/63

1 郭建亭.国际航空,1981;(1) :46
2 郭建亭.能源材料通讯,1984;2(2) :8
3 Hasegawa M, Takeshita K. Metall Trans, 1978; 9B: 383
4 Shaffer T B. Handbooks of High-Temperature Materials. №1: Material Index, New York: Plenum Press. 1964: 165.
5 张匀,赵洪恩,郭建亭.陈桂云.能源材料通讯,1984;2(4) :28&
[1] SI Yongli, XUE Jintao, WANG Xingfu, LIANG Juhua, SHI Zimu, HAN Fusheng. Effect of Cr Addition on the Corrosion Behavior of Twinning-Induced Plasticity Steel[J]. 金属学报, 2023, 59(7): 905-914.
[2] SHEN Zhao, WANG Zhipeng, HU Bo, LI Dejiang, ZENG Xiaoqin, DING Wenjiang. Research Progress on the Mechanisms Controlling High-Temperature Oxidation Resistance of Mg Alloys[J]. 金属学报, 2023, 59(3): 371-386.
[3] LIU Laidi, DING Biao, REN Weili, ZHONG Yunbo, WANG Hui, WANG Qiuliang. Multilayer Structure of DZ445 Ni-Based Superalloy Formed by Long Time Oxidation at High Temperature[J]. 金属学报, 2023, 59(3): 387-398.
[4] RUI Xiang, LI Yanfen, ZHANG Jiarong, WANG Qitao, YAN Wei, SHAN Yiyin. Microstructure and Mechanical Properties of a Novel Designed 9Cr-ODS Steel Synergically Strengthened by Nano Precipitates[J]. 金属学报, 2023, 59(12): 1590-1602.
[5] XU Wenguo, HAO Wenjiang, LI Yingju, ZHAO Qingbin, LU Bingyu, GUO Heyi, LIU Tianyu, FENG Xiaohui, YANG Yuansheng. Effects of Trace Aluminum and Titanium on High Temper-ature Oxidation Behavior of Inconel 690 Alloy[J]. 金属学报, 2023, 59(12): 1547-1558.
[6] SUN Rongrong, YAO Meiyi, LIN Xiaodong, ZHANG Wenhuai, QIU Yunlong, HU Lijuan, XIE Yaoping, YANG Jian, DONG Jianxin, CHENG Guoguang. Effect of Ti on the Corrosion Behavior of Fe22Cr5Al3Mo Alloy in 500oC Superheated Steam[J]. 金属学报, 2022, 58(5): 610-622.
[7] LIN Xiaodong, MA Haibin, REN Qisen, SUN Rongrong, ZHANG Wenhuai, HU Lijuan, LIANG Xue, LI Yifeng, YAO Meiyi. Corrosion Behaviors of Fe13Cr5Al4Mo Alloy in High-Temperature High-Pressure Water Environments[J]. 金属学报, 2022, 58(12): 1611-1622.
[8] LIU Guanxi, HUANG Guanghong, LUO Xuekun, SHEN Zaoyu, HE Limin, LI Jianping, MU Rende. The Influence of Surface Shot Peening on the Isothermal Oxidation Behavior of NiCrAlYSi Coating[J]. 金属学报, 2021, 57(5): 684-692.
[9] YANG Liang, LV Haotian, WAN Chunlei, GONG Qianming, CHEN Hao, ZHANG Chi, YANG Zhigang. Review: Mechanism of Reactive Element Effect—Oxide Pegging[J]. 金属学报, 2021, 57(2): 182-190.
[10] LU Bin, CHEN Furong, ZHI Jianguo, GENG Ruming. Enhanced Welding Properties of High Strength Steel via Rare Earth Oxide Metallurgy Technology[J]. 金属学报, 2020, 56(9): 1206-1216.
[11] GAO Xiang, ZHANG Guikai, XIANG Xin, LUO Lizhu, WANG Xiaolin. Effects of Alloying Elements on the Adsorption of Oxygen on V(110) Surfaces: A First-Principles Study[J]. 金属学报, 2020, 56(6): 919-928.
[12] QIAN Yue,SUN Rongrong,ZHANG Wenhuai,YAO Meiyi,ZHANG Jinlong,ZHOU Bangxin,QIU Yunlong,YANG Jian,CHENG Guoguang,DONG Jianxin. Effect of Nb on Microstructure and Corrosion Resistance of Fe22Cr5Al3Mo Alloy[J]. 金属学报, 2020, 56(3): 321-332.
[13] YAO Meiyi,ZHANG Xingwang,HOU Keke,ZHANG Jinlong,HU Pengfei,PENG Jianchao,ZHOU Bangxin. The Initial Corrosion Behavior of Zr-0.75Sn-0.35Fe-0.15Cr Alloy in Deionized Water at 250 ℃[J]. 金属学报, 2020, 56(2): 221-230.
[14] BAO Feiyang, LI Yanfen, WANG Guangquan, ZHANG Jiarong, YAN Wei, SHI Quanqiang, SHAN Yiyin, YANG Ke, XU Bin, SONG Danrong, YAN Mingyu, WEI Xuedong. Corrosion Behaviors and Mechanisms of ODS Steel Exposed to Static Pb-Bi Eutectic at 600 and 700 ℃[J]. 金属学报, 2020, 56(10): 1366-1376.
[15] Tongbang AN,Jinshan WEI,Jiguo SHAN,Zhiling TIAN. Influence of Shielding Gas Composition on Microstructure Characteristics of 1000 MPa Grade Deposited Metals[J]. 金属学报, 2019, 55(5): 575-584.
No Suggested Reading articles found!