GROWTH OF LARGE SINGLE CRYSTAL Cu FOR NEUTRON MONOCHROMATOR USE |
XUE Bai;LIU Jun Deportment of Physfcs;University of Science and Technology of China;Hefei;ZHANG Taiyong;ZHENG Zhaobo University of Science and Technology of China; Hefei |
|
Cite this article:
XUE Bai;LIU Jun Deportment of Physfcs;University of Science and Technology of China;Hefei;ZHANG Taiyong;ZHENG Zhaobo University of Science and Technology of China; Hefei. GROWTH OF LARGE SINGLE CRYSTAL Cu FOR NEUTRON MONOCHROMATOR USE. Acta Metall Sin, 1988, 24(1): 60-62.
|
Abstract Growth of large single crystal Cu by Bridgman-Stockbarer method was reported.The conditions of growth are: temperature gradient at the level of melting temperature=10℃/cm;the lowering speed of crucible=7-12cm/h. The size of the largest crystal is: diameter=4.1cm; length=18cm; weight=2.1 kg
|
Received: 18 January 1988
|
1 Dorner B. Coherent Inelastic Neutron Scattering in Lattice Dynamics, Berlin: Springer-Verlag, 1982, Chapt. 2. 1 2 Wernick J H. Davis H M. J Appl Phys, 1956; 27: 149. 3 Bacon G E,谈洪,乐 英译.中子衍射,北京:科学出版社,1980:72,95 4 Modrzejewski A, Kobla J. Krist Teeh, 1969; 4: 13 |
No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|