A UNIVERSAL METHOD FOR X-RAY QUANTITATIVE PHASE ANALYSIS WITHOUT STANDARD
ZHANG Xizhang Institute of Metal Research; Academia Sinica; ShenyangLIN Shuzhi Associate professor;Institute of Metal Reseorch; Academia sinice;Shenyang
Cite this article: 

ZHANG Xizhang Institute of Metal Research; Academia Sinica; ShenyangLIN Shuzhi Associate professor;Institute of Metal Reseorch; Academia sinice;Shenyang. A UNIVERSAL METHOD FOR X-RAY QUANTITATIVE PHASE ANALYSIS WITHOUT STANDARD. Acta Metall Sin, 1988, 24(1): 123-128.

Download:  PDF(448KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Based on the works of Zevin and Guo, a quantitative phase analysismethod without standard has been developed. Calculation of absorption coefficientof the sample and addition of extra phase are not necessary. In spite of the num-ber of phases in the sample, only the interesting phases are analysed. The composi-tion is expressed by diffraction intensities from different phases in the same sam-ple, thus, errors caused by the difference between different samples and experimen-tal conditions will be avoided.
Key words:  X-ray      phase quantitative analysis     
Received:  18 January 1988     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1988/V24/I1/123

1 Zevin L S. J Appl Ctystallogr, 1977; 10: 147
2 #12
3 林树智,金属学报,1979;15:266--273
4 林树智,张喜章,金属学报,1985;21:B100
5 刘沃垣,物理,1979;8:224
6 郭常霖,姚公达,物理学报,1985;34:1451
7 姚公达,郭常霖,物理学报,1985;34:1461
8 Klug H P. Alexander L E. X-Ray Diffraction Procedures for Polycrystalline and Amorophous Materials. 2nd ed., New York: wiley, 1974: 532
9 Chung F H. J Appl Crystallogr, 1975; 8: 17
10 陈阴浩,全国X射线衍射无标定量相分析学术讨论会论文摘要汇编,桂林,1986:C-24
[1] LI Shilei, LI Yang, WANG Youkang, WANG Shengjie, HE Lunhua, SUN Guang'ai, XIAO Tiqiao, WANG Yandong. Multiscale Residual Stress Evaluation of Engineering Materials/Components Based on Neutron and Synchrotron Radiation Technology[J]. 金属学报, 2023, 59(8): 1001-1014.
[2] ZHAO Yafeng, LIU Sujie, CHEN Yun, MA Hui, MA Guangcai, GUO Yi. Critical Inclusion Size and Void Growth in Dual-Phase Ferrite-Bainite Steel During Ductile Fracture[J]. 金属学报, 2023, 59(5): 611-622.
[3] ZENG Qiaoshi, YIN Ziliang, LOU Hongbo. Polyamorphic Transitions in Metallic Glasses[J]. 金属学报, 2021, 57(4): 491-500.
[4] LI Yizhuang,HUANG Mingxin. A Method to Calculate the Dislocation Density of a TWIP Steel Based on Neutron Diffraction and Synchrotron X-Ray Diffraction[J]. 金属学报, 2020, 56(4): 487-493.
[5] LI Changji,ZOU Minjie,ZHANG Lei,WANG Yuanming,WANG Sucheng. High-Resolution X-Ray Diffraction Analysis of Epitaxial Films[J]. 金属学报, 2020, 56(1): 99-111.
[6] Huadong YAN,Hui JIN. Three-Dimensional Characteristics and Morphological Evolution of Micro/Meso Pores inG20Mn5N Steel Castings[J]. 金属学报, 2019, 55(3): 341-348.
[7] Zhe SONG, Shengchuan WU, Yanan HU, Guozheng KANG, Yanan FU, Tiqiao XIAO. The Influence of Metallurgical Pores on Fatigue Behaviors of Fusion Welded AA7020 Joints[J]. 金属学报, 2018, 54(8): 1131-1140.
[8] Weifeng HE, Xiang LI, Xiangfan NIE, Yinghong LI, Sihai LUO. Study on Stability of Residual Stress Induced by Laser Shock Processing in Titanium Alloy Thin-Components[J]. 金属学报, 2018, 54(3): 411-418.
[9] Yutuo ZHANG,Cong LI,Pei WANG,Dianzhong LI. IN SITU SYNCHROTRON X-RAY DIFFRACTION INVESTIGATION ON TENSILE PROPERTIES OF 9Ni STEEL[J]. 金属学报, 2016, 52(4): 403-409.
[10] Tao JING, Sansan SHUAI, Mingyue WANG, Qiwei ZHENG. RESEARCH PROGRESS ON 3D DENDRITE MORPHO-LOGY AND ORIENTATION SELECTION DURING THE SOLIDIFICATION OF Mg ALLOYS: 3D EXPERIMENTAL CHARACTERIZATION AND PHASE FIELD MODELING[J]. 金属学报, 2016, 52(10): 1279-1296.
[11] Cheng BI, Zhipeng GUO, E LIOTTI, Shoumei XIONG, P S GRANT. QUANTIFICATION STUDY ON DENDRITE FRAGMENTATION IN SOLIDIFICATION PROCESS OF ALLUMINUM ALLOYS[J]. 金属学报, 2015, 51(6): 677-684.
[12] YU Cheng, WU Shengchuan, HU Yanan, ZHANG Weihua, FU Yanan. THREE-DIMENSIONAL IMAGING OF GAS PORES IN FUSION WELDED Al ALLOYS BY SYNCHROTRON RADIATION X-RAY MICROTOMOGRAPHY[J]. 金属学报, 2015, 51(2): 159-168.
[13] Shenghua ZHANG,Pei WANG,Dianzhong LI,Yiyi LI. INVESTIGATION OF TRIP EFFECT IN ZG06Cr13Ni4Mo MARTENSITIC STAINLESS STEEL BY IN SITU SYNCHROTRON HIGH ENERGY X-RAY DIFFRACTION[J]. 金属学报, 2015, 51(11): 1306-1314.
[14] WANG Shaogang, WANG Sucheng,ZHANG Lei. APPLICATION OF HIGH RESOLUTION TRANSMISSION X-RAY TOMOGRAPHY IN MATERIAL SCIENCE[J]. 金属学报, 2013, 49(8): 897-910.
[15] WAN Qian, ZHAO Haidong,ZOU Chun. THREE-DIMENSIONAL CHARACTERIZATION ANDDISTRIBUTION OF MICROPORES IN ALUMINUMALLOY HIGH PRESSURE DIE CASTINGS[J]. 金属学报, 2013, 49(3): 284-290.
No Suggested Reading articles found!