KINETICS OF INTERACTION OF PbO, xPbO·SiO_2 WITH PbS AND ACTIVITY OF PbO
LIU Chunpeng Kunming College of Engineering LU Yuehua Post Graduate Student for Ph.D.;Department of Metallurgicel;Kunming Institute of Technology
Cite this article: 

LIU Chunpeng Kunming College of Engineering LU Yuehua Post Graduate Student for Ph.D.;Department of Metallurgicel;Kunming Institute of Technology. KINETICS OF INTERACTION OF PbO, xPbO·SiO_2 WITH PbS AND ACTIVITY OF PbO. Acta Metall Sin, 1988, 24(1): 119-122.

Download:  PDF(330KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The rate equation for the reaction of PbO with PbS in liquidstate at 850--1000℃ has been determined as dα/dt=4.73×10~6 exp (-190/RT)in which the activation en ergy E=190kJ/mol. In the solid-liquid reaction system of xPbO. SiO_2-PbS, the rate equation maybe formulated as following: dF(α)/dt=k′(t<20min)+k"(t>20min) (1000℃)where F(α)=α-(N°_(SiO_2/N°_(PbO))ln(1-α) The activities of PbO and SiO_2 in the silicate calculated from the rate dataare in good agreement with those measured thermodynamically.
Key words:  solid-liquid interfacial reaction      chemical control      diffusion control      activity of PbO     
Received:  18 January 1988     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1988/V24/I1/119

1 #12
2 Shohu H Y,Wodsworth M E.郑蒂基译. 提取冶金速过程,北京:冶金工业出版社,1984:153
3 李振家,芦爱春,孙萼庭.全国第一届冶金过程物理化学学术论文集,上海科学技术出版社,1962:380
4 Liou Chunpen, Feng Ganming, Yan Chuanyi, Ho Aiping, First China-USA Bilateral Mctallurgical Conference, Beijing, 1981: 137
5 Richardson F D. WebbL E. Bull Inst Met. 1955; 64: 529
6 Kozuka Z, Samis C S. Met Trans, 1970; 1: 8717
[1] Lei WANG,Di TANG,Yong SONG. AUSTENITE TRANSFORMING IN CONTINUOUS COOLING PROCESS UNDER DIFFUSION CONTROL MODEL[J]. 金属学报, 2015, 51(11): 1341-1348.
[2] Wang Kuangfei. Numerical simulaton of cellular/dendritic transition and its growth during unidirectional solidificationin of Ti–Al alloy[J]. 金属学报, 2007, 43(2): 211-216 .
[3] LI Cheng Beijing Central Engineering and Reseorch Institute for Non-Ferrous Metallurgical Industry; LIU Chunpeng Kunming Institute of Technology. KINETICS OF INTERACTION BETWEEN PbS AND PbO·SiO_2[J]. 金属学报, 1991, 27(1): 145-147.
No Suggested Reading articles found!