| 共析转变过程中内耗与复模量行为的对比 |
| 刘军民;张进修 |
| 中山大学 |
|
| BHAVIOUR OF COMPLEX ELASTIC MODULUS AND INTERNAL FRICTION DURING EUTECTOID DECOMPOSITION |
| LIU Junmin; ZHANG Jinxiu (Zhongshan University; Guangzhou 510275)(Manuscript received 1995-08-09; in revised form 1996-04-11) |
引用本文:
刘军民;张进修. 共析转变过程中内耗与复模量行为的对比[J]. 金属学报, 1996, 32(8): 785-790.
,
.
BHAVIOUR OF COMPLEX ELASTIC MODULUS AND INTERNAL FRICTION DURING EUTECTOID DECOMPOSITION[J]. Acta Metall Sin, 1996, 32(8): 785-790.
| 1ZhangJX,PungPCW,ZengWG.PhysRev,1995;B52:268ZhangJX,YangZY,FungPCW.PhysRev,1995;B52:2782DelormeJF,SchidR,RobinR,GobinP.JPhysColloq,1971;32(C2):1013DejongheW,BatistDR,DeleayL.ScrMetall,1976;10:11254王业宁,杨正举,祝和,马进超.南京大学学报(自然科学版),1963;2:15马应良,葛庭燧.物理学报,1963;20:7216张进修,罗来忠.物理学报,1988;37:353,3637WangYN,ChenXiaohua,ShenHuimin.In:KeTSed.,ProcIntConfonInternalFrictionandUltrasonicAttenuationinSolids,Beijing:AcademicPublishers,1989:3058BidauxJE,SchalierR,BenoitW.ActaMetall,1989;37:8039LiuHY,JonesH.ActaMetallMater,1992;40:200310NuttalK.JInstMet,1971;99:26611TorisakaY,KojimaS.ActaMetallMater,1991;39:94712刘军民,张进修.物理学报,待发表13NowickAS,BerryBS.AnelasticRelaxationinCrystallineSolids.NewYork:AcademicPress,1972:24714HermidaEB.PhysStatusSolidi,1993;B178:371 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|