    					| 新一代的溶液几何模型及其今后的展望 | 
  					 
  					  										
						| 周国治 | 
					 
															
					| 北京科技大学;北京100083 | 
					 
										
						 | 
					 
   										
    					| NEW GENERATION SOLUTION GEOMETRICAL MODEL AND ITS FURTHER DEVELOPMENT | 
  					 
  					  					  					
						| ZHOU Guozhi(Kuo-Chih Chou) (University of Science and Technology Beijing;Beiing 100083) | 
					 
														 
				
				引用本文: 
				
								周国治. 新一代的溶液几何模型及其今后的展望[J]. 金属学报, 1997, 33(2): 126-132.	
																												 																								 . 
				NEW GENERATION SOLUTION GEOMETRICAL MODEL AND ITS FURTHER DEVELOPMENT[J]. Acta Metall Sin, 1997, 33(2): 126-132.	                                                        				  
				
				
					
						
							
								
									
									
									
									
									 
          
          
            
                         
            
									            
									                
																														  
																  1 Kohler Monatsh.Chem, 1960; 91:738 2 Bonnier E Caboz R.Compt,Rend, 1960; 250:527 3 Toop G W.Trans AIME 1965;233: 850 4 Colinet C,D.E.S, Fac Sci,Univ Grenoble,France,(1967) 5 Muggianu Y M,Gambino M,Bros J-P.J Chim Phys(Paris),1965;72:83 6 Jacob K J, Fitzner K. Thermochim Acta, 1973; 18:197 7 Ansaral Int Met Rev,1979 (1): 20 8 Hillert M.CALPHAD 1980; 4(1):1 9 Luck L,Gening U, Predel B. Z Metalkde,1986; 77: 442 10 周国治. 全同第四届熔盐化学和电化学会议文集、郑州,1987 11 Chou K C. CALPHAD, 1987;11(2):123 12 李瑞青,北京科技人学硕士学位论文,1988 13 Chen S L, Chou K C.Rare Met,1989; 8(4): 22 14 Chou K C, Li R Q.Rare Met, 1989;8(4):12 15 Li R Q.CALPHAD, 1989;13(1):67 16 Chen S L,Chou K C. CALPHAD, 1989 13(1):79 17 Chen S L,Cui J Q.Chen T K,Chou K C.CALPHAD,1989; 13(3):225 18  Chou K C, Chang Y A Ber Bunsen-Ges Phys Chem, 1989 93: 741 19 Chou K C.J General Geometrical Model, CALPHAD XXIII-CAMSE 94,Madison,Wisconsin,USA, 1994 20  Chou K C. A New Solution Model For Predicting Thermodynamic Properties of Multicompouent System From Binaries, CALPHAD XXIV95,Kyoto,1995 21 Chou K C. CALPHAD,1995;19(3):315 22 Chou K C et al.Metall Mater Trans.(to be published) | 
															   
																													 
									             
									           
             
			            			 
			 
             
												
											    	
											        	 | 
											        	Viewed | 
											         
													
											        	 | 
											        	 | 
											         
											      	
												         | 
												        
												        	Full text 
												          	
												         | 
											        	
												        	
												        	 
												        	
												          	 
												          	
												          	
														 | 
													 
													
												         | 
												         | 
													 
													
												         | 
												        
												        	Abstract 
												          	
														 | 
												        
															
															 
															
															
												         | 
													 
													
												         | 
												         | 
													 
													
												         | 
												        Cited  | 
												        
												        	
												         | 
													 
													
												         | 
												         | 
												         | 
													 
													
													    |   | 
													    Shared | 
													       | 
												  	 
												  	
													     | 
													     | 
													     | 
											  		 
											  		
													    |   | 
													    Discussed | 
													       | 
												  	 
											 
											 
             
           
      
									
									
		
									
									
									
									
									
									 | 
								 
							 
						 | 
					 
				 
			
		 |