| 纳米反应法制备超细低碳含量Bi-Pb-Sr-Ca-Cu-O超导体原始粉末 |
| 毛传斌;周廉;吴晓祖;杜泽华 |
| 西北有色金属研究院;宝鸡;721014;东北大学;沈阳;110006;西北有色金属研究院;宝鸡;721014;西北有色金属研究院;宝鸡;721014;西北有色金属研究院;宝鸡;721014 |
|
| NANO-REACTION PROCESS TO SYNTHESIZE ULTRAFINE Bi-Pb-Sr-Ca-Cu-O SUPERCONDUCTOR PRECURSOR POWDER WITH LOW CARBON CONTENT |
| MAO Chuanbin;ZHOU Lian;WU Xiaozu;DU Zehua(Northwestern Institute for Nonferrous Metal Research; Baoji 721014)(Northeastern University; Shenyang;110006) |
引用本文:
毛传斌;周廉;吴晓祖;杜泽华. 纳米反应法制备超细低碳含量Bi-Pb-Sr-Ca-Cu-O超导体原始粉末[J]. 金属学报, 1997, 33(5): 533-538.
,
,
,
.
NANO-REACTION PROCESS TO SYNTHESIZE ULTRAFINE Bi-Pb-Sr-Ca-Cu-O SUPERCONDUCTOR PRECURSOR POWDER WITH LOW CARBON CONTENT[J]. Acta Metall Sin, 1997, 33(5): 533-538.
1 Flukiger R,Jeremie A,Hensel B,Seibt E,Xu J Q,Yamada Y.Adv Cryog Eng,1922;38:1073 2 Bhargave A, Yamashita T,Mackinnon I D.Physica C,1995;247:385 3 Wang L N,Zakharchenko I V,Muhammed M,Xu J H,Grisnin A M,Rao K V,Balachandran U.Supercond Sci Technol, 1995;8:94 4 Mao C B,Du Z H,Zhou L.Sci Chin,(Series E),1996;39:182 5梁敬魁,车广灿,陈小龙.高Tc氧化物超导体系的相关系和晶体结构.北京:科学出版社,1994:215 6 Teremie A,Almami-Yadri K,Grivel J C,Flukiger K F.Supercond Sci Technol,1994;6:73 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|