| 钇和硅对Ni_3Al基IC6合金组织和性能的影响 |
| 韩雅芳;肖程波 |
| 北京航空材料研究院;;北京;100095;北京航空材料研究院;;北京;100095 |
|
| EFFECT OF YTTRIUM AND SILICON ON MICROSTRUCTURE AND PROPERTIES OF Ni_3Al BASE ALLOY IC6 |
| HAN Yafang;XIAO Chengbo (Beijing institute of Aeronautical Materials; Beliing 100095) |
引用本文:
韩雅芳;肖程波. 钇和硅对Ni_3Al基IC6合金组织和性能的影响[J]. 金属学报, 1998, 34(11): 1153-1157.
,
.
EFFECT OF YTTRIUM AND SILICON ON MICROSTRUCTURE AND PROPERTIES OF Ni_3Al BASE ALLOY IC6[J]. Acta Metall Sin, 1998, 34(11): 1153-1157.
1Han Y F,Xing Z P,Chaturvedi M C.In:Nathal M V et al eds,Structural Intermetallics,1997:713 2 Pfeil L B. U.K.Patent No.459848,1937 3Kuenzly J D,Douglass D L.Oxid Met,1974;8:139 4 Guo J T; Sun C, Li H, Lai W H, Tan M H,Wang S H.In:Guan H R et al eds,Proc Inter Symposiumon High Temperature Corrosion and Protection.Liaoning Science and Technology Press,1991;45 5王淑荷,郭建亭,李辉,孙超,谭明晖,赖万慧金属学报,1991;27: A433(Wang S H, Guo J T, Li H, Sun C, Tan M H, Lai W H Acta Metall Sin, 1991; 27: A433) 6 Miner R V, Lowell C E. NASA TN D— 7989; 1975 7 Santoro G J et al. NASA TN D- 6414, 1971 8 Lowell C E, Santoro G J. NASA TN D 6838; 19729 Lowed C E, Miner R V. NASA TM- X-68191, 1973 10 Eiselstein H L.Advances in the technology of Stainless Steels and Related Alloys,Disc Philadelpohia,ASTM,1965:78 11 Rizzo F J, Buzzanell J D.J Met, 1969; 21(10): 24 12肖程波,韩雅芳金属学报,1998;34:1158(Xia C B, Han Y F. Acta Metall Sin, 1998; 34: 1158) 13 Xiao C B,Han Y F. Proceedings of 3rd Intermational Workshop on Ordered Intermetawllic Alloys andComposites, 1998; to be published |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|