| 钇提高Ni_3Al基合金IC6氧化皮/基体粘着力的机制 |
| 肖程波;韩雅芳 |
| 北京航空材料研究院;北京;100095;北京航空材料研究院;北京;100095 |
|
| MECHANISM OF IMPROVING THE COHERENCE BETWEEN OXIDE SCALE AND SUBSTRATE OF Ni_3Al BASE ALLOY IC6 BY YTTRIUM |
| XIAO Chengbo;HAN Yafang (Beijing institute of Aeronautical Materials; Beijing 100095) |
引用本文:
肖程波;韩雅芳. 钇提高Ni_3Al基合金IC6氧化皮/基体粘着力的机制[J]. 金属学报, 1998, 34(11): 1158-1162.
,
.
MECHANISM OF IMPROVING THE COHERENCE BETWEEN OXIDE SCALE AND SUBSTRATE OF Ni_3Al BASE ALLOY IC6 BY YTTRIUM[J]. Acta Metall Sin, 1998, 34(11): 1158-1162.
1 PfeilL B U K、Patent No.459848,1937 2McDonald J E,Eberhart J G.Trans Metall Soc AIME,1965;233:512 3Funkenbusch A W,Smeggil J G,Bormsten N S.Metall Trans A,1985;16A(6):1164 4 Alexander J. mater Sci Tech,1985;1(2):167 5Antill J E,Peakall K A.J Iron STeel Inst, 1967;205:1136 6 Francies J M,Juston J A、Corros Sci,1968;8:445 7 Tien J K, Pettit F S Metall Trans, 1972 3: 1587 8 Allam I A,Whittle D P, Stringer J. Oxid Met;1978;12:35 9 Kuenzly J D, Douglass D L.Oxid Met,1974;8:139 10Lustmann B Trans Metall Soc AIME,1950;188:995 11Wukusick C S,Collins J F.Mater Res Stand,1964;4:637 12Huntz A M.In:Lang E ed.The Role of Active Elements in Oxidation Behaviour of Metals and Alloys. Elsevier Applied Science,London/New York,1989:81 13 Jedlinski J.In:Lang E ed.The Role of Active Elements in the Oxidation Behaviour of High Temperature Metals and Alloys Elsevier Applied Science, London, 1989: 131 14 Guo J T,Sun C,Li H, Lai W H,Tan M H,Wang S H. In:Guan H R et al eds,Proceedings of the International Symposium on High Temperature Corrosion and Protection.Liaoning Science and Technology Press, 1991: 45 15王淑荷,郭建亭,李辉,孙超,谭明晖、赖万慧.金属学报、1991;27:A433(Wang S H,Guo J T,Li H,Sun C,Tan M H,Lai W H.Acta Metall Sin,1991 27:A433) 16肖程波.韩雅芳材料工程,1998;(6):23(Xiao C B, Han Y F.J Mater, Eng, 1998;(6): 23)I |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|