| 测定金属薄膜屈服强度的纳米压入法研究 |
| 马德军;徐可为;何家文 |
| 西安交通大学金属材料强度国家重点实验室;西安;710049;西安交通大学金属材料强度国家重点实验室;西安;710049;西安交通大学金属材料强度国家重点实验室;西安;710049 |
|
| A NEW METHOD ON EVALUATING THE YIELD STRENGTH OF METAL FILMS USING DEPTH-SENSING INDENTATION INSTRUMENT |
| MA Dejun; XU Kewei; HE Jiawen(State Key Laboratory for Mechanical Behavior of Materials; Xi'an Jiaotong University Xi'an 710049)Corespondent :HE Jiawen; professor Tel: (029)3268696; For: (029)32379910;E-mail: jwheoritu.edu.cn |
引用本文:
马德军;徐可为;何家文. 测定金属薄膜屈服强度的纳米压入法研究[J]. 金属学报, 1998, 34(6): 661-666.
,
,
.
A NEW METHOD ON EVALUATING THE YIELD STRENGTH OF METAL FILMS USING DEPTH-SENSING INDENTATION INSTRUMENT[J]. Acta Metall Sin, 1998, 34(6): 661-666.
1 Blech I A.J Appl Phpo, 1976; 47: 1203 2 Arz E,Nix W D.J Mater Res ,1991;6:731 3 Reed D T, Dally J W.J Mater Rea, 1993; 8: 1542 4 Shute C J, Cohen J B.J Mater Res, 1991; 6: 950 5 Beder S, Kalaugher E M, Ant E. Thin Solid Films , 1995; 263: 175 6 Murakami Y, Yuan L, P.J Test Eval, 1992; 20: 15 7 Wissmann J W, Hauch C. Comput Struct., 1983; 17:8 8 Lee C H Murakami S,Kobayaahi S.Int J Mech Sci 1972 ;14:417 9 Field J S, Swain M V.J Mater Res, 1995; 10(1): 101 10 Field J S, Swain M V.J Mater Res, 1993; 8: 297+ |
|