| Ti处理改善船体钢焊接粗晶区的低温韧性研究 |
| 杨银辉1;2;3); 柴锋2); 严彪1;3); 苏航2); 杨才福2) |
1) 同济大学材料科学与工程学院; 上海 200092
2) 钢铁研究总院结构材料研究所; 北京 100081
3) 同济大学上海市金属功能材料开发应用重点实验室; 上海 200092 |
|
| STUDY ON LOW TEMPERATURE TOUGHNESS IMPROVEMENT OF WELDING COARSE GRAIN ZONE OF HULL STEELS BY Ti TREATMENT |
| YANG Yinhui1;2;3); CHAI Feng2) ; YAN Biao1;3); SU Hang2); YANG Caifu2) |
1) School of Materials Science and Engineering; Tongji University; Shanghai 200092
2) Institute of Structure Materials; Central Iron and Steel Research Institute; Beijing 100081
3) Shanghai Key Lab of D$\&$A for Metal-Functional Materials; Tongji University; Shanghai 200092 |
引用本文:
杨银辉 柴锋 严彪 苏航 杨才福. Ti处理改善船体钢焊接粗晶区的低温韧性研究[J]. 金属学报, 2010, 46(1): 62-70.
.
STUDY ON LOW TEMPERATURE TOUGHNESS IMPROVEMENT OF WELDING COARSE GRAIN ZONE OF HULL STEELS BY Ti TREATMENT[J]. Acta Metall Sin, 2010, 46(1): 62-70.
| [1] Lee J L. Acta Metall, 1994; 42: 3291
[2] Tomita Y, Saito N, Tsuzuki T, Tokunaga Y, Okamoto K. ISIJ Int, 1994; 34: 829
[3] Song F M, Li Z G, Qian Y H, Shen K. Hot Work Technol, 2006; 35(19): 69
(宋凤明, 李自刚, 钱余海, 沈凯. 热加工工艺, 2006; 35(19): 69)
[4] Chen M A, Wu C S, Yang M, Tang Y M, Wu R J. Acta Metall Sin, 2004; 40: 148
(陈茂爱, 武传松, 杨 敏, 唐逸民, 吴人洁. 金属学报, 2004; 40: 148)
[5] Yamamoto K, Hasegawa T, Takamura J–I. ISIJ Int, 1996; 36: 80
[6] Rlcks R A, Howell P R, Barritte G S. J Mater Sci, 1982; 17: 732
[7] Ishikawa F, Takahashi T, Ochi T. Metall Mater Trans, 1994; 25A: 929
[8] Madariaga I, Romero J L, Guti´errez I. Metall Mater Trans, 1998; 29A: 1003
[9] Lee T–K, Kim H J, Kang B Y, Hwang S K. ISIJ Int, 2000; 40: 1260
[10] Dowling J M, Corbett J M, Kerr H W. Metall Trans, 1986; 17A: 1611.
[11] Shim J H, Oh Y J, Suh J Y, Cho Y W, Shim J D, Byun J S, Lee D N. Acta Mater, 2001; 49: 2115
[12] Kim H–S, Lee H–G, Oh K–S. ISIJ Int, 2002; 42: 1404
[13] Byun J S, Shim J H, Cho Y W, Lee D N. Acta Mater, 2003; 51: 1593
[14] Shim J H, Cho Y W, Chung S H, Shim J D, Lee D N. Acta Mater, 1999; 47: 2751
[15] TianDW, Qian B N, Chen X F, Si C Y. Phys Test Chem Anal–Phys Test, 1994; 30(1): 28
(田德蔚, 钱百年, 陈晓风, 斯重遥. 理化检验--物理分册, 1994; 30(1): 28)
[16] Chen Y T, GuoAM, Wu L X, Zeng J, Li P H. Acta Metall
Sin (Engl Lett), 2006; 19: 65
[17] Fang H S, Bai B Z, Zheng X H, Zheng Y K, Chen X Y, Zhao R F. Acta Metall Sin, 1986; 22: A283
(方鸿生, 白秉哲, 郑秀华, 郑燕康, 陈秀云, 赵如发. 金属学报, 1986; 22: A283)
[18] Chai F, Yang C F, Zhang Y Q, Xu Z. J Iron Steel Res, 2005; 17(1): 42
(柴锋, 杨才福, 张永权, 徐 洲. 钢铁研究学报, 2005; 17(1): 42)
[19] Fang H S, Liu D Y, Xu P G, Bai B Z, Yang Z G. Mater Mech Eng, 2001; 25(6): 1
(方鸿生, 刘东雨, 徐平光, 白秉哲, 杨志刚. 机械工程材料, 2001; 25(6): 1)
[20] Yong Q L. The Second Phase in Iron & Steel. Beijing: Metallurgical Industry Press, 2006: 49
(雍岐龙. 钢铁材料中的第二相. 北京: 冶金工业出版社, 2006: 49) |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|