| 横向磁场对镍基高温合金定向凝固组织的影响 |
| 董建文; 任忠鸣; 任维丽; 李喜; 李旭 |
| 上海大学上海市现代冶金与材料制备重点实验室; 上海 200072 |
|
| EFFECT OF HORIZONTAL MAGNETIC FIELD ON THE MICROSTRUCTURE OF DIRECTIONALLY SOLIDIFIED Ni-BASED SUPERALLOY |
| DONG Jianwen; REN Zhongming; REN Weili; LI Xi; LI Xu |
| Shanghai Key Laboratory of Modern Metallurgy $\&$ Materials Processing; Shanghai University; Shanghai 200072 |
引用本文:
董建文 任忠鸣 任维丽 李喜 李旭. 横向磁场对镍基高温合金定向凝固组织的影响[J]. 金属学报, 2010, 46(1): 71-76.
,
,
,
,
.
EFFECT OF HORIZONTAL MAGNETIC FIELD ON THE MICROSTRUCTURE OF DIRECTIONALLY SOLIDIFIED Ni-BASED SUPERALLOY[J]. Acta Metall Sin, 2010, 46(1): 71-76.
| [1] Matthiesen D H, Wargo M J, Motakef S, Carlson D J, Nakos J S, Witt A F. J Cryst Growth, 1987; 85: 557
[2] Robertson G D Jr, Oconner D J. J Cryst Growth, 1986; 76: 100
[3] Yang S, Liu W J. Mater Sci, 2001; 36: 5351
[4] Tewari S N, Shah R, Song H. Metall Mater Trans, 1994; 25A: 1535
[5] Li X, Fautrelle Y, Ren Z M. Acta Mater, 2007; 55: 3803
[6] Liu Z Y, Yang A M, Li J G, Shi Z X, Fu H Z. Mater Sci Prog, 1992; 6: 481
(刘忠元, 杨爱民, 李建国, 史正兴, 傅恒志. 材料科学进展, 1992; 6: 481)
[7] Zhang N, Lin J P, Wang Y L, Chen G L. Aeronaut Mater, 2006; 26: 42
(张宁, 林均品, 王艳丽, 陈国良. 航空材料学报, 2006; 26: 42)
[8] Ren W L, Zhang T, Ren Z M, Zhao A K, Zhong Y B, Guo J T. Mater Lett, 2009; 63: 382
[9] Utech H P, Flemings, M C. J Appl Phys, 1966; 37: 2021
[10] Alboussiere T, Moreau R, Camel D. C R Acad Sci, 1991; 313: 749
[11] Lehmann P, Moreau R, Camel D, Bolcato R. Acta Mater, 1998; 46: 4067
[12] Li X, Gagnoud A, Ren Z M, Fautrelle Y, Moreau R. Acta Mater, 2009; 57: 2180
[13] Moore J J, Shah N A. Met Rev, 1983; 28: 338
[14] Garandet J P, Alboussiere T. Prog Cryst Growth Charact Mater, 1999; 38: 100
[15] Lehmann P, Moreau R, Camel D, Bolcato R. J Cryst Growth, 1998; 183: 690
[16] Dupouy M D, Camel D, Favier J J. Acta Metall Mater, 1992; 40: 1791 |
|