| 激光原位制备复合碳化物颗粒增强铁基复合涂层及其耐磨性的研究 |
| 吴朝锋;马明星;刘文今;钟敏霖;张伟明;张红军 |
| 清华大学机械工程系先进成形制造教育部重点实验室; 北京 100084 |
|
| STUDY ON WEAR RESISTANCE OF LASER CALDDING Fe–BASED COMPOSITE COATINGS REINFORCED BY IN–SITU MULTIPLE CARBIDE PARTICLES |
| WU Chaofeng; MA Mingxing; LIU Wenjin; ZHONG Minlin; ZHANG Weiming; ZHANG Hongjun |
| Key Laboratory for Advanced Materials Processing Technology; Ministry of Education; Department of Mechanical Engineering; Tsinghua University; Beijing 100084 |
引用本文:
吴朝锋 马明星 刘文今 钟敏霖 张伟明 张红军. 激光原位制备复合碳化物颗粒增强铁基复合涂层及其耐磨性的研究[J]. 金属学报, 2009, 45(8): 1013-1018.
,
,
,
,
,
.
STUDY ON WEAR RESISTANCE OF LASER CALDDING Fe–BASED COMPOSITE COATINGS REINFORCED BY IN–SITU MULTIPLE CARBIDE PARTICLES[J]. Acta Metall Sin, 2009, 45(8): 1013-1018.
| [1] Yang S, Zhong M L, Liu W J. Mater Sci Eng, 2003; A343: 57
[2] Wang X H, Song S L, Zou Z D, Qu S Y. Mater Sci Eng, 2006; A441: 60
[3] Park H, Nakata K, Tomida S. J Mater Sci, 2000; 35: 747
[4] Singh A, Dahotre N B. J Mater Sci, 2004; 39: 4553
[5] Zhang Q M, He J J, Liu W J, Zhong M L. Laser Technol, 2003; 27(2): 81
(张庆茂, 何金江, 刘文今, 钟敏霖. 激光技术, 2003; 27(2): 81)
[6] Ma M X, Liu W J, Zhong M L, Wu C F, Zhang W M, Zhang H J. Chin J Lasers, 2007; 34(Supll): 1
(马明星, 刘文今, 钟敏霖, 吴朝锋, 张伟明, 张红军. 中国激光, 2007; 34(增刊): 1)
[7] Zhang J Y, Ma M X, Liu W J, Zhong M L, Zhang W M, Zhang H J. Heat Treat Met, 2003; 28(8): 1
(张锦英, 马明星, 刘文今, 钟敏霖, 张伟明, 张红军. 金属热处理, 2003; 28(8): 1)
[8] Ma M X, Liu W J, Zhong M L, Zhu Y H, Wang H L, Zhang W M, Zhang H J. Appl Laser, 2006; 26: 145
(马明星, 刘文今, 钟敏霖, 朱有慧, 王海龙, 张伟明, 张红军. 应用激光, 2006; 26: 145)
[9] Wu C F, Ma M X, Liu W J, Zhong M L, Zhang W M, Zhang H J. Procedings of ICALEO, Orlando: Laser Institute of America, 2007: 940
[10] Qu S Y,Wang X H, Zhang M, Zou Z D. J Mater Sci, 2008; 431546
[11] Wang X H, Zhang M, Liu X M, Qu S Y, Zou Z D. Sur Coat Technol, 2008; 202: 3600
[12] Cui C Y, Guo Z X, Wang H Y, Hu H D. J Mater ProcessTechnol, 2007; 183: 380
[13] Ma M X. PhD Thesis, Tsinghua University, Beijing, 2006
(马明星. 清华大学博士学位论文, 北京, 2006)
[14] Qian Z Y, Zhong M L, Liu W J, Ma M X, Zhang H J. Chin J Lasers, 2008; 35: 1271
(钱兆勇, 钟敏霖, 刘文今, 马明星, 张红军. 中国激光, 2008; 35: 1271) |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|