金属学报  2009, Vol. 45 Issue (8): 1013-1018    
  论文 本期目录 | 过刊浏览 |
激光原位制备复合碳化物颗粒增强铁基复合涂层及其耐磨性的研究
吴朝锋;马明星;刘文今;钟敏霖;张伟明;张红军
清华大学机械工程系先进成形制造教育部重点实验室; 北京 100084
STUDY ON WEAR RESISTANCE OF LASER CALDDING Fe–BASED COMPOSITE COATINGS REINFORCED BY IN–SITU MULTIPLE CARBIDE PARTICLES
WU Chaofeng; MA Mingxing; LIU Wenjin; ZHONG Minlin; ZHANG Weiming; ZHANG Hongjun
Key Laboratory for Advanced Materials Processing Technology; Ministry of Education; Department of Mechanical Engineering; Tsinghua University; Beijing 100084
引用本文:

吴朝锋 马明星 刘文今 钟敏霖 张伟明 张红军. 激光原位制备复合碳化物颗粒增强铁基复合涂层及其耐磨性的研究[J]. 金属学报, 2009, 45(8): 1013-1018.
, , , , , . STUDY ON WEAR RESISTANCE OF LASER CALDDING Fe–BASED COMPOSITE COATINGS REINFORCED BY IN–SITU MULTIPLE CARBIDE PARTICLES[J]. Acta Metall Sin, 2009, 45(8): 1013-1018.

全文: PDF(2273 KB)  
摘要: 

通过在高碳当量铁基熔覆粉末中复合添加多种强碳化物形成元素, 激光原位制备的颗粒增强铁基复合材料涂层具有颗粒析出密度大、尺寸分布均匀的优点. 通过在铁基熔覆粉末中单独添加Ti, 复合添加Ti+Zr以及Ti+Zr+WC的方式, 运用激光熔覆技术在中碳钢表面制备了颗粒增强铁基复合涂层. 用X射线衍射仪、扫描电镜和透射镜等手段研究了涂层的显微组织、颗粒相结构及颗粒相与熔覆层基体相之间的界面. 通过环块磨损实验, 对比渗碳淬火工艺研究了颗粒增强涂层的耐磨性能, 并对磨损机制进行了讨论.结果表明, 涂层微观结构是典型的亚共晶介稳组织, 原位合成的颗粒是一种复合碳化物, 界面处结合牢固. 激光原位制备复合碳化物颗粒增强铁基复合涂层具有优异的耐磨性能.

关键词 激光熔覆 颗粒增强 复合碳化物 铁基复合涂层 耐磨性    
Abstract

Particle reinforced metal matrix composites (PR–MMCs) have attracted extensive investigation in material science and engineering. They combine both strength and toughness and show excellent properties such as good wear resistance, corrosion resistance and high temperature properties. Laser depositing of metal matrix composite coatings containing in–situ carbide particles is a research focus in laser surface processing. The essential advantage of the in–situ synthesis technology is that the reinforcements are much more compatible with the matrix and the interface between the reinforcements and the matrix is much cleaner. It has a special advantage in high distribution density and dimension uniformity to in–situ synthesize particles by laser melting precursor powders containing several strong carbide-forming elements (SCFEs) rather than one. Each SCFE has significant effects on the precipitation and distribution of the carbide particles. To investigate the microstructure and properties of the cladded ayers, in this paper, the coatings were produced by laser cladding powders containing 2%Ti, 1%Ti+1%Zr and 1%Ti+1%Zr+10%WC (mass fraction) respectively on the surface of a medium carbon steel. The microstructure of the coatings and the carbide particles were studied by X–ray diffractometer (XRD), scanning electron microscopy (SEM) and transmission electron microscopy (TEM). The results show that the microstructure of the coatings is typically hypo–eutectic. The in–situ particles have a TiC structure with high content of Zr or W when 1%Ti+1%Zr and 1%Ti+1%Zr+10%WC are added into the cladded powders. Therefore, they are multiple carbides. The interface between the article and the ae material is strong. The optimized istribution of the particles with high distribution density (2×104 mm−2) and high dimension uniformity (about 1μm) are obtained when 1%Ti+1%Zr+10%WC are added. The wear resistance of the coating was tested throgh ring–on–block wear eperiment. It is indicated that laser cladding Fe–based composite coating reinforced by in–situ multiple carbide particles presents excellent wear resistance.

Key wordslaser cladding    particle reinforced    mutipe carbide    Fe–based composite coating    wear reitance
收稿日期: 2009-01-20     
ZTFLH: 

TN249

 
基金资助:

国际科技合作计划(专项经费)资助项目2007DFA50870

作者简介: 吴朝锋, 男, 1982年生, 博士生

[1] Yang S, Zhong M L, Liu W J. Mater Sci Eng, 2003; A343: 57
[2] Wang X H, Song S L, Zou Z D, Qu S Y. Mater Sci Eng, 2006; A441: 60
[3] Park H, Nakata K, Tomida S. J Mater Sci, 2000; 35: 747
[4] Singh A, Dahotre N B. J Mater Sci, 2004; 39: 4553
[5] Zhang Q M, He J J, Liu W J, Zhong M L. Laser Technol, 2003; 27(2): 81
(张庆茂, 何金江, 刘文今, 钟敏霖. 激光技术, 2003; 27(2): 81)
[6] Ma M X, Liu W J, Zhong M L, Wu C F, Zhang W M, Zhang H J. Chin J Lasers, 2007; 34(Supll): 1
(马明星, 刘文今, 钟敏霖, 吴朝锋, 张伟明, 张红军. 中国激光, 2007; 34(增刊): 1)
[7] Zhang J Y, Ma M X, Liu W J, Zhong M L, Zhang W M, Zhang H J. Heat Treat Met, 2003; 28(8): 1
(张锦英, 马明星, 刘文今, 钟敏霖, 张伟明, 张红军. 金属热处理, 2003; 28(8): 1)
[8] Ma M X, Liu W J, Zhong M L, Zhu Y H, Wang H L, Zhang W M, Zhang H J. Appl Laser, 2006; 26: 145
(马明星, 刘文今, 钟敏霖, 朱有慧, 王海龙, 张伟明, 张红军. 应用激光, 2006; 26: 145)
[9] Wu C F, Ma M X, Liu W J, Zhong M L, Zhang W M, Zhang H J. Procedings of ICALEO, Orlando: Laser Institute of America, 2007: 940
[10] Qu S Y,Wang X H, Zhang M, Zou Z D. J Mater Sci, 2008; 431546
[11] Wang X H, Zhang M, Liu X M, Qu S Y, Zou Z D. Sur Coat Technol, 2008; 202: 3600
[12] Cui C Y, Guo Z X, Wang H Y, Hu H D. J Mater ProcessTechnol, 2007; 183: 380
[13] Ma M X. PhD Thesis, Tsinghua University, Beijing, 2006
(马明星. 清华大学博士学位论文, 北京, 2006)
[14] Qian Z Y, Zhong M L, Liu W J, Ma M X, Zhang H J. Chin J Lasers, 2008; 35: 1271
(钱兆勇, 钟敏霖, 刘文今, 马明星, 张红军. 中国激光, 2008; 35: 1271)

[1] 冯凯, 郭彦兵, 冯育磊, 姚成武, 朱彦彦, 张群莉, 李铸国. 激光熔覆高强韧铁基涂层精细组织调控与性能研究[J]. 金属学报, 2022, 58(4): 513-528.
[2] 赵万新, 周正, 黄杰, 杨延格, 杜开平, 贺定勇. FeCrNiMo激光熔覆层组织与摩擦磨损行为[J]. 金属学报, 2021, 57(10): 1291-1298.
[3] 童文辉, 张新元, 李为轩, 刘玉坤, 李岩, 国旭明. 激光工艺参数对TiC增强钴基合金激光熔覆层组织及性能的影响[J]. 金属学报, 2020, 56(9): 1265-1274.
[4] 张林, 郭晓, 高建文, 邓安元, 王恩刚. 电磁搅拌对TiB2颗粒增强钢组织和力学性能的影响[J]. 金属学报, 2020, 56(9): 1239-1246.
[5] 张煜, 娄丽艳, 徐庆龙, 李岩, 李长久, 李成新. 超高速激光熔覆镍基WC涂层的显微结构与耐磨性能[J]. 金属学报, 2020, 56(11): 1530-1540.
[6] 董虎林,包海萍,彭建洪. TiC含量对铁基复合材料力学性能及耐磨性能的影响[J]. 金属学报, 2019, 55(8): 1049-1057.
[7] 范丽, 陈海龑, 董耀华, 李雪莹, 董丽华, 尹衍升. 激光熔覆铁基合金涂层在HCl溶液中的腐蚀行为[J]. 金属学报, 2018, 54(7): 1019-1030.
[8] 林英华, 袁莹, 王梁, 胡勇, 张群莉, 姚建华. 电磁复合场对Ni60合金凝固过程中显微组织和裂纹的影响[J]. 金属学报, 2018, 54(10): 1442-1450.
[9] 童文辉,赵子龙,张新元,王杰,国旭明,段新华,刘豫. 球墨铸铁表面激光熔覆TiC/钴基合金组织和性能研究[J]. 金属学报, 2017, 53(4): 472-478.
[10] 何波,聂庆武,张洪宇,韦华. 固溶处理对CoCrW合金组织及耐磨性能的影响*[J]. 金属学报, 2016, 52(4): 484-490.
[11] 刘彬,贡凯,乔岩欣,董世运. 基于金属磁记忆评价裂纹埋深对激光熔覆层应力的影响*[J]. 金属学报, 2016, 52(2): 241-248.
[12] 徐滨士,方金祥,董世运,刘晓亭,闫世兴,宋超群,夏丹. FV520B不锈钢激光熔覆热影响区组织演变及其对力学性能的影响*[J]. 金属学报, 2016, 52(1): 1-9.
[13] 刘晓波, 赵宇光. 不同制备条件下原位Mg2Si/Al复合材料的组织演变和耐磨性*[J]. 金属学报, 2014, 50(6): 753-761.
[14] 林英华, 雷永平, 符寒光, 林健. 激光原位制备硼化钛与镍钛合金增强钛基复合涂层[J]. 金属学报, 2014, 50(12): 1513-1519.
[15] 林英华, 雷永平, 符寒光, 林健. Ni添加对TiB2/TiB钛基复合涂层组织与力学性能的影响[J]. 金属学报, 2014, 50(12): 1520-1528.