| 过共析钢温变形过程中的组织演变 II. 渗碳体的球化及Al的影响 |
| 陈伟1;李龙飞1;杨王玥2;孙祖庆1;张艳1 |
1. 北京科技大学新金属材料国家重点实验室; 北京 100083
2. 北京科技大学材料科学与工程学院; 北京 100083 |
|
| MICROSTRUCTURE EVOLUTION OF HYPEREUTECTOID STEELS DURING WARM DEFORMATION II. Cementite Spheroidization and Effects of Al |
| CHEN Wei 1; LI Longfei 1; YANG Wangyue 2; SUN Zuqing 1; ZHANG Yan 1 |
1. State Key Laboratory for Advanced Metals and Materials; University of Science and Technology Beijing;Beijing 100083
2. School of Materials Science and Engineering; University of Science and Technology Beijing; Beijing 100083 |
引用本文:
陈伟 李龙飞 杨王玥 孙祖庆 张艳. 过共析钢温变形过程中的组织演变 II. 渗碳体的球化及Al的影响[J]. 金属学报, 2009, 45(2): 156-160.
,
,
,
,
.
MICROSTRUCTURE EVOLUTION OF HYPEREUTECTOID STEELS DURING WARM DEFORMATION II. Cementite Spheroidization and Effects of Al[J]. Acta Metall Sin, 2009, 45(2): 156-160.
| [1] Sherby O D, Walser B, Young C M, Cady E M. Scr Metall, 1975; 9: 569
[2] Sherby O D, Oyama T, Kum D W, Walser B, Wadsworth J. J Met , 1985; 37(6): 50
[3] Oyama T, Sherby O D, Wadsworth J, Walser B. Scr Metall, 1984; 18: 799
[4] Furuhara T, Mizoguchi T, Maki T. ISIJ Int , 2005; 45: 392
[5] Lesuer D R, Syn C K, Goldberg A, Wadsworth J, Sherby O D. JOM, 1993; 45(8): 40
[6] Syn C K, Lesuer D R, Goldberg A, Tsai H C, Sherby O D. Mater Sci Forum, 2007; 539--543: 4844
[7] Chattopadhyay S, Sellars C M. Acta Metall, 1982; 30: 157
[8] Robbins J L, Shepard O C, Sherby O D. J Iron Steel Inst, 1964; 202: 804
[9] Harrigan M J, Sherby O D. Mater Sci Eng, 1971; 7: 177
[10] Paqueton H, Pineau A. J Iron Steel Inst, 1971; 209: 991
[11] Kaspar R, Kapellner W, Lang C. Steel Res, 1988; 59: 492
[12] Peng H F, Song X Y, Gao A G, Ma X L. Mater Lett, 2005; 59: 3330
[13] Lesuer D R, Syn C K, Whittenberger J D, Sherby O D. Metall Mater Trans, 1999; 30A: 1559
[14] Frommeyer G, Jimenez J A. Metall Mater Trans, 2005; 36A: 295
[15] Tsuzaki K, Sato E, Furimoto S, Furuhara T, Maki T. Scr Mater, 1999; 40: 675
[16] Fukuyo H, Tsai H C, Oyama T, Sherby O D. ISIJ Int, 1991; 31: 76
[17] Hernandez D, Jimenez, J A, Frommeyer G. Mater Trans, 1996; 37: 1758
[18] Chen W, Li L F, Yang W Y, Sun Z Q. Acta Metall Sin, 2009; 45: 151
(陈伟, 李龙飞, 杨王玥, 孙祖庆. 金属学报, 2009; 45: 151)
[19] Chen G A, Yang W Y, Sun Z Q. Acta Metall Sin, 2007; 43: 27
(陈国安, 杨王玥,孙祖庆. 金属学报, 2007; 43: 27)
[20] Chen W, Li L F, Yang W Y, Sun Z Q. Chin J Mater Res, 2008; 22: 374
(陈 \ \ 伟, 李龙飞, 杨王玥,孙祖庆. 材料研究学报, 2008; 22: 374)
[21] Huang Q S, Li L F, Yang W Y, Sun Z Q. Acta Metall Sin,2007; 43: 724
(黄青松, 李龙飞, 杨王玥,孙祖庆. 金属学报, 2007; 43: 724)
[22] Chen W, Li L F, Yang W Y, Sun Z Q. Acta Metall Sin,2008; 44: 626
(陈 \ \ 伟, 李龙飞, 杨王玥,孙祖庆. 金属学报, 2008; 44: 626)
[23] Song R, Ponge D, Raabe D, Kaspar R. Acta Mater, 2005; 53: 845
[24] Chen G A, Yang W Y, Sun Z Q, Zhang X Y. Acta Metall Sin,2007; 43: 785
(陈国安, 杨王玥,孙祖庆, 张湘义. 金属学报, 2007; 43: 785)
[25] Gavriljuk V G. Mater Sci Eng, 2003; A345: 81
[26] Li L F, Yang W Y, Sun Z Q. Acta Metall Sin, 2003; 39: 419
(李龙飞, 杨王玥,孙祖庆. 金属学报, 2003; 39: 419)
[27] Wang B Q, Song X Y, Peng H F. Mater Des,2007; 28: 562
[28] Zuidema B K, Subramaanyam, Leslie W C. Metall Trans, 1987; 18A: 1629
[29] Laxar B F H, Frame J W, Blickwede D J. Trans ASM, 1961; 53: 683
[30] Leslie W C, Rauch G C. Metall Trans, 1978; 9A: 343 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|