| 溶质截留对过冷共晶生长过程的影响 |
| 赵素;李金富;刘礼;周尧和 |
| 上海交通大学材料科学与工程学院 |
|
| Effect of solute trapping on the growth process in undercooled eutectic melts |
| ;;;Yaohe Zhou |
| 上海交通大学 |
引用本文:
赵素; 李金富; 刘礼; 周尧和 . 溶质截留对过冷共晶生长过程的影响[J]. 金属学报, 2008, 44(11): 1335-1339 .
,
,
,
.
Effect of solute trapping on the growth process in undercooled eutectic melts[J]. Acta Metall Sin, 2008, 44(11): 1335-1339 .
[1]Jackson K A,Hunt J D.TMS AIME,1966;236:1129 [2]Trivedi R,Magnin P,Kurz W.Acta Metall,1987;35:971 [3]Li J F,Zhou Y H.Sci China,2005;35E:449 (李金富,周尧和.中国科学,2005;35E:449) [4]Kurz W,Trivedi R.Metall Trans,1991;22A:3051 [5]Li J F,Zhou Y H.Acta Mater,2005;53:2351 [6]Aziz M J.J Appl Phys,1982;53:1158 [7]Sobolev S L.Phys Rev,1997;55E:6845 [8]Wang H,Liu F,Chen Z,Yang G,Zhou Y.Acta Mater, 2007;55:497 [9]Wang H,Liu F,Yang W,Chen Z,Yang G,Zhou Y.Acta Mater,2008;56:746 [10]Goetzinger R,Barth M,Herlach D M.J Appl Phys,1998; 84:1643 [11]Li J F,Jie W Q,Zhao S,Zhou Y H.Metall Mater Trans, 2007;38A:1806 [12]Lipton J,Glicksman M E,Kurz W.Mater Sci Eng,1984; 65:57 [13]Trivedi R,Kurz W.Acta Metall,1986;34:1663 [14]Boettinger W J,Coriell S R,Trivedi R.In:Mehrabian R, Parrish P A,eds,,Rapid Solidification Processing:Prin- ciple and Technologies,Baton Rouge:Claitors,1987:13 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|