| 凸形多面体个体晶粒的三维von Neumann准确方程 |
| 王浩;刘国权 |
| 北京科技大学材料科学与工程学院 |
|
| AN EXACT THREE-DIMENSIONAL VON NEUMANN RELATION FOR INDIVIDUAL CONVEX POLYHEDRON GRAINS |
| ; |
| 北京科技大学 |
引用本文:
王浩; 刘国权 . 凸形多面体个体晶粒的三维von Neumann准确方程[J]. 金属学报, 2008, 44(11): 1332-1334 .
,
.
AN EXACT THREE-DIMENSIONAL VON NEUMANN RELATION FOR INDIVIDUAL CONVEX POLYHEDRON GRAINS[J]. Acta Metall Sin, 2008, 44(11): 1332-1334 .
[1]von Neumann J.In:Herring C,ed.,Metal Interfaces, Cleveland:American Society for Metals,1952:108 [2]Mullins W W.J Appl Phys,1956;27:900 [3]Rhines F N,Craig K R.Metall Trans,1974;5:413 [4]Rivier N.Philos Mag,1983;47B:L45 [5]Hillert M.Acta Metall,1965;13:227 [6]Glazier J A.Phys Rev Lett,1993;70:2170 [7]Yu H B,Liu G Q.China Sci Bull,1996;41:2000 (于海波,刘国权.科学通报,1996;41:2000) [8]Liu G Q,Yu H B,Song X Y,Qin X G.Mater Design, 2001;22:33 [9]Liu G Q,Song X Y,Yu H B,Gu N J.Acta Metall Sin, 1999;35:245 (刘国权,宋晓艳,于海波,谷南驹.金属学报,1999;35:245) [10]Hilgenfeldt S,Kraynik A M,Koehler S A,Stone H A.Phys Rev Lett,2001;86:2685 [11]Hilgenfeldt S,Kraynik A M,Reinelt D A,Sulliwan J M. Europhys Lett,2004;67:484 [12]Liu G Q,Yu H B,Song X Y,Qin X G,Wang C.J Univ Sci Technol Beijing,2004;11:212 [13]Glicksman M E.Mater Sci Forum,2004;467-470:1025 [14]Glicksman M E.Philos Mag,2005;85:3 [15]Wang H,Liu G Q.Acta Metall Sin,2008;44:13 (王浩,刘国权.金属学报,2008;44:13) [16]MacPherson R D,Srolovitz D J.Nature,2007;446:1053 [17]Kinderlehrer D.Nature,2007;446:995 [18]DeHoff R T.In:Braun J D,Arrowsmith H W,McCall J L,eds.,Microstructural Science,New York:Elsevier North-Holland,1977;5:331 [19]DeHoff R T,Liu G Q.Metall Trans,1985;16A:2007 [20]Hilliard J E.In:Elias H,ed.,Stereology,New York: Springer-Verlag,1967:221 [21]DeHoff R T.Acta Metall Mater,1994;42:2633 [22]Minknowski H.Math Ann,1903;57:447 [23]Kendall M G,Moran P A P.Geometrical Probability.Lon- don:Charles Griffin,1963:81 [24]Struik D J.Lectures on Classical Differential Geometry, New York:Addison-Wesley,1950:25 [25]Taylor J E.Acta Metall Mater,1992;40:1475 [26]Rios P R,Fonseca G S,Lins J F C,Augusto F P M.Scr Mater,2007;57:727 [27]Liu G Q,Yu H B,Qin X G.Mater Sci Eng,2002;A326: 276 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|