Please wait a minute...
金属学报  2007, Vol. 43 Issue (11): 1176-1180     
  论文 本期目录 | 过刊浏览 |
溶质扩散控制层片共晶生长
孟广慧 林 鑫 黄卫东
西北工业大学凝固技术国家重点实验室
Lamellar Eutectic Growth Controlled By Solute Diffusion
MENG Guanghui; LIN Xin; HUANG Weidong
State Key Laboratory of Solidification Processing;Northwestern Polytechnical University
引用本文:

孟广慧; 林鑫; 黄卫东 . 溶质扩散控制层片共晶生长[J]. 金属学报, 2007, 43(11): 1176-1180 .
, , . Lamellar Eutectic Growth Controlled By Solute Diffusion[J]. Acta Metall Sin, 2007, 43(11): 1176-1180 .

全文: PDF(641 KB)  
摘要: 基于平界面溶质扩散假设,改进界面物质守恒边界条件求得层片共晶稳态生长的溶质边界层。结果表明,层片共晶组织生长过程中沿生长方向的溶质边界层与沿界面方向的溶质边界层相关。对于CBr4-C2Cl6透明合金系的分析表明,共晶成分合金,其层片组织生长过程界面处液、固相平均成分的差值随凝固速度的增大而增大。合金成分偏离共晶成分时,界面处液相平均成分与共晶成分非常接近。在给定凝固速度条件下,共晶相界面处液、固相平均成分差值与层片宽度的比值随合金成分变化关系不同。
关键词 : 凝固,  共晶,  扩散,  溶质边界层    
Abstract:Based on the planar assumption, the solute boundary layer in lamellar eutectic growth in steady-state is estimated by means of modifying the conservation of mass at solid/liquid interface. It is found that the solute boundary layer along the growth direction is related to that along the solid/liquid interface. For transparent organic system CBr4-C2Cl6 of eutectic composition, the difference in average composition of the solids and that of the liquid at solid/liquid interface increases with increasing in growth velocities. The average composition in the liquid at solid/liquid interface still closes to the eutectic one as the initial composition of the alloy is apart from the eutectic point. In addition, for a fixed growth rate, the variation of ratio of the difference in average composition to the lamellar widths of the two solid phases with initial composition of the alloy is noticeably distinct.
Key words: solidification    eutectic    diffusion    solute boundary layer
收稿日期: 2007-03-28     
ZTFLH:  TG244  
[1]Hunt J D.Sci Technol Adv Mater,2001;2:147
[2]Karma A,Plapp M.JOM,2004;56:28
[3]Jackson K A,Hunt J D.Trans AIME,1966;236:1129
[4]Ma D,Jie W Q.Acta Metall Sin,1996;32:791 (马东,介万奇.金属学报,1996;32:791)
[5]Datye V,Langer J S.Phys Rev,1981;24B:4155
[6]Ginibre M,Akamatsu S,Faivre G.Phys Rev,1997;56E: 780
[7]Magnin P,Kurz W.In:Stefanescu D M ed,Metals Hund- book Vol.15 Casting.Metals Park,OH:ASM interna- tional,1988:119
[8]Tiller W A,Jackson K A,Rutter J W,Chalmers B.Acta Metall,1953;1:428
[9]Hunt J D.J Cryst Growth,1968;3-4:82
[10]Hunt J D,Shu-Zu Lu,In:Hurle D T.J ed.Handbook of Crystal Growth.Vol.2,Part B:Bulk Crystal Growth: Growth Mechanism and Dynamics,Amsterdam:North Holland,1994:1111
[11]Wilcox W R,Gegel L L.Acta Astronaut,1996;38:51
[12]Ma D,Li Y,Ng S C.J Cryst Growth,2000;219:300
[13]Derby B,Favier J J.Acta Metall,1983;31:1123
[14]Stocker C,Ratke L.J Cryst Growth,2000;212:324
[15]Han S H,Trivedi R.Metall Mater Trans,2000;31A:1819
[16]Karma A,Rappel W J,Fuh B C,Trivedi R.Metall Mater Trans,1998;29A:1457
[17]Kerr H W,Kurz W.Int Mater Rev,1996;41:129
[18]Liu J C,Elliott R.Acta Metall Mater,1995;43:3301
[19]Akamatsu S,Plapp M,Faivre G,Karma A.Phys Rev, 2002;66E:030501(R)
[20]Series R W,Hunt J D,Jackson K A.J Cryst Growth, 1977;40:221
[21]Catalina A V,Sen S,Stefanescu D M.Metall Mater Trans, 2003;34A:383
[22]Magnin P,Trivedi R.Acta Metall Mater,1991;39:453
[23]Seetharaman V,Trivedi R.Metall Trans,1988;19A:2955!
[1] 马德新, 赵运兴, 徐维台, 王富. 重力对高温合金定向凝固组织的影响[J]. 金属学报, 2023, 59(9): 1279-1290.
[2] 宫声凯, 刘原, 耿粒伦, 茹毅, 赵文月, 裴延玲, 李树索. 涂层/高温合金界面行为及调控研究进展[J]. 金属学报, 2023, 59(9): 1097-1108.
[3] 张健, 王莉, 谢光, 王栋, 申健, 卢玉章, 黄亚奇, 李亚微. 镍基单晶高温合金的研发进展[J]. 金属学报, 2023, 59(9): 1109-1124.
[4] 刘继浩, 周健, 武会宾, 马党参, 徐辉霞, 马志俊. 喷射成形M3高速钢偏析成因及凝固机理[J]. 金属学报, 2023, 59(5): 599-610.
[5] 侯娟, 代斌斌, 闵师领, 刘慧, 蒋梦蕾, 杨帆. 尺寸设计对选区激光熔化304L不锈钢显微组织与性能的影响[J]. 金属学报, 2023, 59(5): 623-635.
[6] 苗军伟, 王明亮, 张爱军, 卢一平, 王同敏, 李廷举. AlCr1.3TiNi2 共晶高熵合金的高温摩擦学性能及磨损机理[J]. 金属学报, 2023, 59(2): 267-276.
[7] 胡文滨, 张晓雯, 宋龙飞, 廖伯凯, 万闪, 康磊, 郭兴蓬. 共晶高熵合金AlCoCrFeNi2.1 在H2SO4 溶液中的腐蚀行为[J]. 金属学报, 2023, 59(12): 1644-1654.
[8] 徐文国, 郝文江, 李应举, 赵庆彬, 卢炳聿, 郭和一, 刘天宇, 冯小辉, 杨院生. 微量Al、Ti对Inconel 690合金高温氧化行为的影响[J]. 金属学报, 2023, 59(12): 1547-1558.
[9] 苏震奇, 张丛江, 袁笑坦, 胡兴金, 芦可可, 任维丽, 丁彪, 郑天祥, 沈喆, 钟云波, 王晖, 王秋良. 纵向静磁场下单晶高温合金定向凝固籽晶回熔界面杂晶的形成与演化[J]. 金属学报, 2023, 59(12): 1568-1580.
[10] 刘路军, 刘政, 刘仁辉, 刘永. Nd90Al10 晶界调控对晶界扩散磁体磁性能和微观结构的影响[J]. 金属学报, 2023, 59(11): 1457-1465.
[11] 张丽丽, 吉宗威, 赵九洲, 何杰, 江鸿翔. 亚共晶Al-Si合金中微量元素La变质共晶Si的关键影响因素[J]. 金属学报, 2023, 59(11): 1541-1546.
[12] 李赛, 杨泽南, 张弛, 杨志刚. 珠光体-奥氏体相变中扩散通道的相场法研究[J]. 金属学报, 2023, 59(10): 1376-1388.
[13] 沈莹莹, 张国兴, 贾清, 王玉敏, 崔玉友, 杨锐. SiCf/TiAl复合材料界面反应及热稳定性[J]. 金属学报, 2022, 58(9): 1150-1158.
[14] 梁琛, 王小娟, 王海鹏. 快速凝固Ti-Al-Nb合金B2相形成机制与显微力学性能[J]. 金属学报, 2022, 58(9): 1169-1178.
[15] 冯迪, 朱田, 臧千昊, 李胤樹, 范曦, 张豪. 喷射成形过共晶AlSiCuMg合金的固溶行为[J]. 金属学报, 2022, 58(9): 1129-1140.