| 非晶Ni-P合金镀层压痕塑性变形及氢对塑性变形的影响 |
| 周庆军;何健英;郝小鹏;乔利杰;李金许;褚武扬 |
| 北京科技大学材料物理与化学系 |
|
| THE PLASTIC DEFORMATION AND EFFECT OF HYDROGEN ON DEFORMATION OF Ni-P AMORPHOUS COATINGS |
| Qing-Jun Zhou;;;;; |
| 北京科技大学材料物理与化学系 |
引用本文:
周庆军; 何健英; 郝小鹏; 乔利杰; 李金许; 褚武扬 . 非晶Ni-P合金镀层压痕塑性变形及氢对塑性变形的影响[J]. 金属学报, 2007, 42(1): 87-90 .
,
,
,
,
,
.
THE PLASTIC DEFORMATION AND EFFECT OF HYDROGEN ON DEFORMATION OF Ni-P AMORPHOUS COATINGS[J]. Acta Metall Sin, 2007, 42(1): 87-90 .
[1] Kramer D,Huang H,Kriese M,Robach J,Nelson J, Wright A,Bahr D,Gerberich W W.Acta Mater,1999; 47:333 [2] Vaidyanathan R,Dao M,Ravichandran G,Suresh S. Acta Mater, 2001; 49:3781 [3] Schuh C A,Nieh T G.Acta Mater,2003;5l:87 [4] Jana S,Bhowmick R,Kawamura Y,Chattopadhyay K, Ramamurty U.Intermetallics,2004; 12:1097 [5] Jana S,Ramamurty U,Chattopadhyay K,Kawamura Y. Mater Sci Eng, 2004; A375—377:1191 [6] Greer A L,Castellero A,Madge S V,Walker I T,Wilde J R.Mater Sci Eng, 2004; A375-377:1182 [7] Ramamurty U, Jana S,Kawamura Y,Chattopadhyay K.Acta Mater,2005;53:705 [8] Wu X F,Zhang H F,Li H,Wang A M,Yang H C,Hu Z Q.Chin J Nonferrous Met,2003;13:1368) (武晓峰,张海峰,李宏,王爱民,杨洪才,胡壮麒.中国有色金属学报,2003;13:1368) [9] Lin J J,Perng T P.Metall Mater Trans,1995;26A:197 [10] Namboodhiri T K,Ramesh T A,Singh G,Seghal S. Mater Sci Eng, 1983; 61:23 [11] Suh D,Dauskardt R H.Scr Mater,2000;42:233 [12] Wang Y W,Chu W Y,Li J X,Hui X D,Wang Y B,Gao K W,Qiao L J.Mater Lett,2004; 58:2393 [13] Reidel W.Electroless Nickel Plating.London:Finishing Publications, 1991:1 [14] Zhou Q J,He J Y,Li J X,Chu W Y,Qiao L J.Mater Lett,2006;60:349 [15] Peng X,Su Y J,Gao K W,Qiao L J,Chu W Y.Mater Lett,2004;58:2073 [16] dos Santos D S,de Biasi R S,de Miranda P E V.J Non Cryst Solids, 1997;210:136 [17] Johnson K L.J Mech Phys Solids,1970;18:115 [18] Tao S J.J Chem Phys,1972;56:5499 [19] Eldrup M,Colemal P G.Positron Annihilation.Amster- dam:North—Holland, 1982:1 [20] Hagiwara K,Ougizawa T,Inoue T,Hirata K,Kobayashi Y.Radiat Phys Chem, 2000;58:525T |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|