| 氢对锆基块体非晶合金形变和开裂的影响 |
| 单广斌; 魏炳忱;李金许; 乔利杰; 褚武扬 |
| 北京科技大学腐蚀与防护中心环境断裂实验室; 北京100083 |
|
| Effects of Hydrogen on Shear Bands and Cracking in Zr Base Bulk Amorphous Alloy |
| SHAN Guangbin; WEI Bingchen;LI Jinxu; QIAO Lijie; CHU Wuyang |
| Laboratory of Environmental Fracture; Corrosion and Protection Center; University of Science and Technology Beijing; Beijing 100083 |
引用本文:
单广斌; 魏炳忱; 李金许; 乔利杰; 褚武扬 . 氢对锆基块体非晶合金形变和开裂的影响[J]. 金属学报, 2006, 42(7): 689-693 .
,
,
,
,
.
Effects of Hydrogen on Shear Bands and Cracking in Zr Base Bulk Amorphous Alloy[J]. Acta Metall Sin, 2006, 42(7): 689-693 .
[1] Vaidyanathan R,Dao M,Ravichandran G,Suresh S. Acta Mater, 2001; 49: 3781 [2] Flores K M,Dauskardt R H. Scr Mater, 1999, 41: 937 [3] Spaepen F. Acta Metall, 1977; 25: 407 [4] Inoue A, Zhang W, Zhang T, Kurosaka K. Acta Mater, 2001; 49: 2645 [5] Xing L Q, Li Y, Ramesh K T, Li J, Hufnagel T L.Phys Rev, 2001; 64B: 180201 [6] Wright W J, Schwarz R B, Nix W D. Mater Sci Eng, 2001;A319-321: 229 [7] Flores K M, Dauskardt R H. Acta Mater, 2001; 49: 2527 [8] Li J X, Chu W Y, Gao K W , Qiao L J. Acta Metall Sin,2003; 39: 359 (李金许,褚武扬,高克玮,乔利杰,金属学报,2003;39:359) [9] Li J X, Shan G B, Gao KW,Qiao L J,Chu W Y. Mater Sci Eng, 2003; A354: 337 [10] Namboodhiri T K, Ramesh T A, Singh G,Seghal S. Mater Sci Eng, 1983; 61: 23 [11] Lin J J, Perng T P. Metall Mater Trans,1995; 26A: 197 [12] Suh D, Danskardt R H. Scr Mater, 2000; 42: 233 [13] Guo J X, Li J X, Qiao L J, Gao K W, Chu W Y. Corros Sci, 2003; 45: 735 [14] Eliaz N, Banks-Sills L,Ashkenazi D,Eliasi R. Acta Mater, 2004; 52: 93 [15] Shan G. B, Wang Y W,Chu W Y, Li J X, Hui X D. Corros Sci, 2005; 47: 2731 [16] Peng X, Su Y J,Gao K W,Qiao L J,Chu W Y.Mater Lett, 2004; 58: 2073 [17] Creager M, Paris P C. Int J Fract Mech,1967; 4: 247 [18] Wang Y W, Chu W Y, Li J X, Su Y J, Gao K W, Qiao L J. Mater Lett, 2004; 58: 2393 |
|