| 应力和夹杂对车轮钢中氢鼓泡的影响 |
| 武明; 褚武扬;李金许; 姜波; 陈刚; 崔银会 |
| 北京科技大学材料物理系 |
|
| EFFECT OF STRESS AND INCLUSION ON HYDROGEN BLISTERING |
| ;;;;; |
| 北京科技大学 |
引用本文:
武明; 褚武扬; 李金许; 姜波; 陈刚; 崔银会 . 应力和夹杂对车轮钢中氢鼓泡的影响[J]. 金属学报, 2006, 42(8): 815-819 .
,
,
,
,
,
.
EFFECT OF STRESS AND INCLUSION ON HYDROGEN BLISTERING[J]. Acta Metall Sin, 2006, 42(8): 815-819 .
[1]Chu W Y.Hydrogen Damage and Delayed Cracking.Beijing:Metallurgical Industry Press,1988:146(褚武扬.氢损伤与滞后断裂.北京:冶金工业出版社,1988:146) [2]Smialowski M.Hydrogen in Steel.New York:Pergamon Press,1962:327 [3]Interrante C G.In:Interrante C G,Pressourye G M,eds.,Current Solution to Hydrogen Problems in Steels,Metals Park,OH:ASM,1982:2 [4]Steiner J E.In:Interrante C G,Pressourye G M,eds.,Current Solution to Hydrogen Problems in Steels,Metals Park,OH:ASM,1982:55 [5]Fruehan R J.Iron Steel Maker,1997;24:61 [6]Pressourye G M.In:Interrante C G,Pressourye G M,eds.,Current Solution to Hydrogen Problems in Steels,Metals Park,OH:ASM,1982:18 [7]Oriani R A,Hirth J P,Smialowski M.Hydrogen Degradation of Ferrous Alloys.Park Ridge,N J:Noyes Pub,1985:737 [8]Panagopoulos C N,El-Amoush A S,Agathocleous P E.Corros Sci,1998;40:1837 [9]Ren X C,Shan G B,Chu W Y,Su Y J,Gao K W,QiaoL J.Chin Sci Bull,2005;50:1962 [10]Ren X C,Chu W Y,Li J X,Qiao L J.Acta Metall Sin,2006;42:275 (任学冲,褚武扬,李金许,乔利杰.金属学报,2006;42:275) [11]Chu W Y,Qiao L J,Chen Q Z,Gao K W.Fracture and Environment Fracture.Beijing:Science Press,2001:133 (褚武扬,乔利杰,陈奇志,高克玮.断裂与环境断裂.北京:科学出版社,2001:133) [12]Chu W Y,Li J X,Huang C H,Wang Y B,Qiao L J.Corrosion,1999;55:892 [13]Ren X C,ChuW Y,Li J X,Qiao L J.Acta Metall Sin,2006;42:156 (任学冲,褚武扬,李金许,乔利杰.金属学报,2006;42:156) [14]Peng X,Su Y J,Gao K W,Qiao L J,Chu W Y.Mater Lett,2004;58:2073 [15]Wu M,Ren X C,Chu W Y,Li J X,Qiao L J,Jiang B,Chen G,Cui Y H.Acta Metall Sin,2006;42,in press (武明,任学冲,褚武扬,李金许,乔利杰,江波,陈刚,崔银会.金属学报,2006;42,待发表) [16]Spiegel M R,Schiller J,Srinivasan,R A.Schaum's Outline of Theory and Problems of Probability and Statistics.2nd ed,New York:McGraw-Hill Co,2000:171 [17]Timoshenko S,Gocdier J N.Theory of Elasticity.2nd ed,New York:McGraw-Hill Book Co,1951:375 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|