| Nb对TiNiAl合金高温氧化行为的影响 |
| 徐 舰; 赵新青; 宫声凯; 徐惠彬 |
| 北京航空航天大学 |
|
| THE EFFECT OF Nb ON THE OXIDATION BEHAVIOR OF TiNiAl ALLOYS |
| Xinqing Zhao |
| 北京航空航天大学 |
引用本文:
徐舰; 赵新青; 宫声凯; 徐惠彬 . Nb对TiNiAl合金高温氧化行为的影响[J]. 金属学报, 2006, 42(8): 820-826 .
,
,
,
.
THE EFFECT OF Nb ON THE OXIDATION BEHAVIOR OF TiNiAl ALLOYS[J]. Acta Metall Sin, 2006, 42(8): 820-826 .
[1]Otsuka K,Wayman C M.Shape Memory Materials.London:Cambridge University Press,1998:1 [2]Duerig T W,Melton K N,Proft J L.In:Duerig T W,ed.,Engineering Aspects of Shape Memory Alloys,London:Btterworth-Heinemann,1990:130 [3]Hsieh S F,Wu S K.J Mater Sci,1997;32:989 [4]Ohishi K,Horita Z,Nemoto M.Mater Trans JIM,1997;38:99 [5]Jung J,Ghosh G,Isheim D,Olson G B.Metall Mater Trans,2003;34A:1221 [6]Koizumi Y,Ro Y,Nakazawa S,Harada H.Mater Sci Eng,1997;A233:36 [7]Roy T K,Balasubramaniam R,Ghosh A.Metall Mater Trans,1996;27A:3993 [8]Zeng C L,Li M C,Liu G Q,Wu W T.Oxid Met,2002;58:171 [9]Firstov G S,Vitchev R G,Kumar H,Blanpain B,Humbeeck J Van.Biomaterials,2002;23:4863 [10]Varma S K,Chan A,Mahapatra B N.Oxid Met,2001;55:423 [11]Shida Y,Anada H.Oxid Met,1996;45:197 [12]Sunderkotter J D,Schmutzler H J,Haanappel V A C,Hofman R,Glatz W,Clemens H,Stroosnijder M F.Intermetallics,1997;5:525 [13]Perez P,Haanappel V A C,Stroosnijder M F.Mater Sci Eng,2000;A284:126 [14]Roy T K,Balasubramaniam R,Ghosh A.Metall Mater Trans,1996;27A:4003 [15]Jiang H R,Hirohasi M,Lu Y,Hitoshi I.Scr Mater,2002;46:639 [16]Chu C L,Wu S K,Yen Y C.Mater Sci Eng,1996;A216:195 [17]Li M S.The High Temperature Corrosion of Metals.Beijing:Metallurgical Industry Press.2001:5,63(李美栓.金属的高温腐蚀.北京:冶金工业出版社,2001:5,63) [18]Welsh G,Kahveci A J.In:Grobstein T,Doychat J,eds.,Oxidation of High Temperature Intermetallics,Warrendale,Pennsylvania:The Minerals,Metals and Materials Society,1989:207 [19]Meier G H,Appalonia D.In:Grobstein T,Doychat J,eds.,Oxidation of High Temperature Intermetallics,Warrendale,Pennsylvania:The Minerals,Metals and Materials Society,1989:185 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|