| Al-Pb合金雾化液滴的液-液相变动力学 |
| 赵九洲;高玲玲; 何杰; 王江涛; 陈桂云 |
| 中国科学院金属研究所; 沈阳 110016 |
|
引用本文:
赵九洲; 高玲玲; 何杰; 王江涛; 陈桂云 . Al-Pb合金雾化液滴的液-液相变动力学[J]. 金属学报, 2006, 42(2): 113-117 .
[1] Ratke L, Diefenbach S. Mater Sci Eng, 1995; R15: 263 [2] Lu X Y, Cao C D, Kolbe M, Wei B, Herlach D M. Mater Sci Eng, 2004; A375-377: 1101 [3] Zhao J Z, Ratke L, Feuerbacher B. Modelling Simul Mater Sci Eng, 1998; 6: 123 [4] Zhao J Z, Drees S, Ratke L. Mater Sci Eng, 2000; A282: 262 [5] Guo J J, Liu Y, Jia J, Su Y Q, Ding H S, Zhao J Z, Xue X. Scr Mater, 2001; 45: 1197 [6] Zhao J Z, Ratke L. Scr Mater, 2004; 50: 543 [7] Chen G Y, Tian C, Yang L, Zhao J Z, Zhang Y C. Chin J Mech, 2002; 38(8): 139(陈桂云,田冲,杨林,赵九洲,张永昌.机械工程学报,2002;38(8):139) [8] Grant P S, Cantor B, Katgerman L. Acta Metall Mater, 1993: 41: 3097 [9] Clif R, Grace J R, Weber M E. Bubbles, Drops and Particles. New York: Academic Press, 1978: 111 [10] Ranz W E, Marshall W R. Chem Eng Prog, 1952; 48: 141, 173 [11] Yu S K, Sommer FZ.Z Metallkd, 1996; 87: 574 [12] Davis R H. Zhang X G. Wang H. In: Ratke L ed., Immiscible Metals and Organics, Oberursel: DGM-Informationsgesellschaft, 1993: 163 [13] Christian J. The Theory of Phase Transformation in Metals and Alloys. Vol.1, 2nd ed, Elmsford, NY: Pergamon Press, 1975: 1 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|