| 弹性交互作用下直刃型位错的稳态构型及其滑移稳定性 |
| 于志伟 刘路 关德林 |
| 大连海事大学金属材料研究所; 大连 116026 |
|
引用本文:
于志伟; 刘路; 关德林 . 弹性交互作用下直刃型位错的稳态构型及其滑移稳定性[J]. 金属学报, 1999, 35(4): 348-352 .
[1]Li J C M. Acta Metall, 1960; 8: 296 [2]Divincenzo D P, ROttman C. Phys Rev, 1988; B37: 5242 [3]Feng D. Physics of Metals (Vol.1). Beliing: Science Press,1980: 229(冯端.金属物理学(第一卷). 北京.科学出版社,1980: 229) [4] Koevich A M. In: Nabarro F R N ed., Dislocations in Solids,Vol1, Amsterdam: North-Holland, 1979: 66 [5] Hirth J P, Lothe J. Theory of Dislocations. 2nd ed., NewYork: John Wiley & Sons, 1982: 117 [6] Nabarro F R N. Adv Phys, 1952; 1: 269 [7] Yang S H. Theory Basis of Dislocations in Crystals (Vol. 1).Beijing: Science Press, 1988: 138(杨顺华.晶体位错理论基础(第一卷).北京:科学出版社,1988:138) |
|