| 金属间化合物提高陶瓷接头高温性能的作用 |
| 吴爱萍 邹贵生 |
| 清华大学机械工程系;北京 100084 |
|
引用本文:
吴爱萍; 邹贵生 . 金属间化合物提高陶瓷接头高温性能的作用[J]. 金属学报, 2000, 36(11): 1213-1218 .
[1] Tillmann W, Lugscheider E, Schlimbach K, Manter C, Indacochea J E. Weld J, 1997; 76: 300s [2] Tillmann W, Lugscheider E, Schlimbach K, Manter C, Indacochea J E. Weld J, 1998; 77: 103s [3] Lugscheider E, Tillmann W. Manuf Process, 1993; 8: 219 [4] Miyama K, Ito M, Narita T. J Jpn Inst Met, 1996; 60:497(见山克已,伊藤正也,成田敏夫.日本金属学会志,1996;60:497) [5] Selverian J H, Kang S. Weld J, 1992; 71: 25s [6] Peteves S D, Panlasto M, Ceccone G. Acta Mater 1998;46: 2407 [7] Torrecillas R, Sainz M A, Moya A S. Scr Metall Mater,1994; 31: 1031 [8] Singh M. Adv Mater Processes, 1998; 10: 89 [9] Philip A. J Am Ceram Soc, 1995; 78: 999 [10] Xie R J, Li P H, Yuan C, Fu X R. J Mater Sci, 1999; 34:1783 [11] Salvo M, Ferraris M, Lemoine P, Appendino Montorsi M,Merola M. J Nucl Mater, 1996; 233: 949 [12] Singh M. Scr Mater 1997; 37: 1151 [13] Locatelli M R, Tomsia A P, Nakashima K, Dalgleish B J,Glaeser A M. Key Eng Mater, 1995; 111-112: 157 [14] Shalz M L, Dalgleish B J, Tomsia A P, Glaeser A M. JMater Sci, 1994; 29: 3200 [15] Dalgleish B J, Tomsia A P, Nakashima K, Locatelli M K,Glaeser A M. Scr Metall Mated 1994; 31: 1043 [16] Shalz M L, Dalgleish B J, Tomsia A P, Cannon R M,Glaeser A M. J Mater Sci, 1994; 29: 3678 [17] Chen Z, Lon H Q, Fei Z, Li Z Z. J Mater Sci Lett, 1997;16: 2026 [18] Hansen M, Anderko K. Constitution of Binary Alloy (II).Neywords: McGraw-Hill Book Company, INC, 1958: 807S |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|