| 输入焓对火焰喷涂合成TiC-Fe涂层的影响 |
| 刘长松 刘永合 |
| 北京科技大学材料科学与工程系;北京 100083 |
|
引用本文:
刘长松; 刘永合 . 输入焓对火焰喷涂合成TiC-Fe涂层的影响[J]. 金属学报, 2000, 36(11): 1209-1212 .
[1] Liu C S, Yin S. Mater Prot, 2000; 33: 83(刘长松,殷声.材料保护,2000:33:83) [2] Liu C S, Liu Y H, Yin S. Acta Metall Sin, 2000; 36: 62(刘长松,刘永合,殷声.金属学报,2000;36:62) [3] Munir Z A. Mater Sci Rep, 1989; 3: 277 [4] Jonsson S. Metall Mater Trans, 1998; B29: 361 [5] Jonsson S. Z Metallkd, 1996; 87: 703 [6] Jonsson S. Metall Mater Trans, 1998; B29: 371 [7] Dallaire S, Cliche G. Surf Coat Technol, 1991; 50: 233 [8] M ed. Ma Z C trans. High Refractory Material. Beijing: Metallurgical Industry Press,1984: 18(M著.马志春译.高级耐火复合材料北京:冶金工业出版社,1984:18) |
|