| Fe-Ni-Mo-(Si)-B非晶的晶化及纳米晶合金磁性的研究 |
| 赵玉华 全明秀 陈文智 |
| 东北大学材料科学与工程系;沈阳 110006 |
|
引用本文:
赵玉华; 全明秀; 陈文智 . Fe-Ni-Mo-(Si)-B非晶的晶化及纳米晶合金磁性的研究[J]. 金属学报, 2000, 36(3): 291-294 .
[1] Yoshizawa Y, Oguma S, Yamanchi J. J Appl Phys, 1988; 64:6044 [2] Suzuki K, Kataoka N, Inoue A, Makino A, Masumoto T.Mater Trans JIM, 1990; 31: 743 [3] Yoshizawa Y, Yamauchi K. Mater Sci Eng, 1991; A133: 176 [4] Noh T H, Lee M B, Kim H J, Kang I K. J Appl Phys, 1990;67: 5568 [5] M L Sui, Qian L H, He K Y. Proct 5fth IUMRS Int Conf OnAdvanced Materials, Beijing, 1999 [6] Sui M L, Zhou F, He K Y, Wang R, Cheng L Z. NanostructMater, 1994; 4: 734 [7] Bozorth R M. Ferro-magnetism. New York: Van Nostrand,1951: 104 [8] Abrosinnova G E, Atonin A S, Zver' kova I I, Kit' janov YuV, Molokanov V V, Petrzhik M I. In: Dubai P eds., Proc 9thInt Conf On Rapidly Quenched Metals. Elsevier, 1997: 76k |
|