应变诱发Inconel718合金γ〃相析出和γ〃→δ转变 |
陈宗霖 刘文昌 |
沈阳黎明发动机制造公司; 沈阳 110043 |
|
引用本文:
陈宗霖; 刘文昌 . 应变诱发Inconel718合金γ〃相析出和γ〃→δ转变[J]. 金属学报, 2000, 36(2): 150-154 .
[1] Paulonis D F, Oblak J M, Duvall D S. Trans ASM, 1969; 62:611 [2] Kirman I, Warrington D H. Metall Trans, 1970; Al: 2667 [3] Cozar R, Pineau A. Metall Trans, 1973; A4: 47 [4] Oblak J M, Paulonis D F, Duvall D S. Metall Trans, 1974;A5: 143 [5] Sundararaman M, Mukhopadhyay P, Banerjee S. MetallTrans, 1988; A19: 453 [6] Sundararaman M, Mukhopadhyay P, Banerjee S. MetallTrans, 1992; A23: 2015 [7] Slama C, Servant C, Cizeron G. J Mater Res, 1997; 12: 2289 [8] Han Y F, Deb P, Chaturvddi M C. Metall Sci, 1982; 16: 555 [9] Kuasabiraki K, Wang L, Ooka T, Yamada K. Iron Steel,1990; 76: 1341. [10] Wlodek S T, Field R D. In: Loria E A ed, Superalloys 718,625, 706 and Various Derivatives, Warrendale, PA, TMS,1994: 659 [11] Dong J X, Xie X S, Zhang S H. Scr Metall, 1995; 33: 1933 [12] Dong J X, Xie X S, Xu Z C, Zhang S H. In: Loria E A ed,Saperalloys 718, 625, 706 and Various Derivatives, Warren-dale, PA, TMS, 1994: 649 [13] Singh R P, Hyzak J M, Howson T E, Biederman R R. In:Loria E A ed, Superalloys 718, 625 and Various Derivatives,Warrendale, PA, TMS, 1991: 205 [14] Burger J L, Biederman R R, Couts W H. In: Loria E A ed,Saperolloy 718 - Metallurpy and Applications, Warrendale,PA, TMS, 1989: 207 [15] Liu W C, Xiao F R, Yao M, Chen Z L. J Mater Sci Lett,1997; 16: 769 [16] Avrami M. J Chem Phys, 1940; 8: 212 [17] Liu W C, Xiao F R, Yao M, Chen Z L. J Mater Sci Lett,1998; 17: 245 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|