| Ti-47Al-2W-0.5Si抗蠕变合金的高温力学行为和变形机制 |
| 周兰章 郭建亭 V.Lupinc M.Maldini |
| 中国科学院金属研究所;沈阳 110016 |
|
引用本文:
周兰章; 郭建亭; V.Lupinc; M.Maldini . Ti-47Al-2W-0.5Si抗蠕变合金的高温力学行为和变形机制[J]. 金属学报, 2001, 37(8): 785-790 .
[1] Appel F, Wagner R. Mater Sci Eng, 1998; 22R: 187 [2] Lupinc V, Yin W M, Maldini M. In: Jacqueline L B, Flo-rian S, Philip J E eds., Materials for Advanced PowerEngineering 1998, Liege: University de Liege, EuropeanCommission, 1998: 1239 [3] Kim Y W, Dimiduk D M. J Met, 1991; 43: 40 [4] Beddoes J, Wallace W, Zhao L. Int Mater Rev, 1995; 40:197 [5] Kim Y W. J Met, 1994; 46: 30 [6] Beddoes J, Zhao L, Au P, Dudzinski D, Triaotafillou. In:Nathal M V, Miracle D B, Wagner R, Yamaguchi M eds.,Structural Intermetallics 1997 Warrandale, PA: The Min-erals, Metals & Materials Society 1997: 109 [7] Chen G L, Zhang L C, Zhang W J. Intermetallics, 1999;7: 1211 [8] Zhang W J, Evangelista E, Francesconi L. Mater Sci Eng,1996: 220A: 15 [9] Zhang Y G, Han Y F, Chen G L, Guo J T, Wan X J,Feng D eds., Structural Intermetallics, Beijing: NationalDefence Industry Press, 2001: 705(张永刚,韩雅芳,陈国良,郭建亭,万晓景,冯 涤主编 金属间化合物结构材料 北京:国防工业出版社,2001:705 [10] Nazmy M, Staubli M. US Pat, 5286443, 1994; 5207982,1993; 5342577, 1994. EU Pat 45505 B1 [11] Yin W M, Lupinc V, Battezzati L. Mater Sci Eng, 1997;239-240A: 713 [12] Yin W M, Lupinc V. Scr Maten 1997; 37: 211 [13] Yu R, He L L, Jin Z X, Guo J T, Ye H Q, Lupinc V. ZMetallkd, 2000; 4: 91 [14] Yin W M, Guo J T, Lupinc V. Acta Metall Sin, 1999; 35:32(殷为民,郭建亭,Lupinc V. 金属学报, 1999; 35: 32) [15] Yin W M, Guo J T, Lupinc V. Acta Metall Sin, 1999; 35:37(殷为民,郭建亭, Lupinc V. 金属学报, 1999; 35: 37) [16] Naxmy M, Lupinc V. In: Jacqueline L B, Florian S, PhilipJ E eds., Materials for Advanced Power Engineering 1998,Liege: University de Liege, European Commission, 1998:933 [17] Morris M A, Leboeuf M. Mater Sci Eng, 1997; 239-240A:429 [18] Hayes R W, Mcquay P A. Scr Metall Maten 1994; 30:259 [19] Hsiung L M, Nieh T G. Mater Sci Eng, 1997; 239-240A:438 [20] Du X W, Zhu J, Zhang X, Cheng Z Y, Kim Y W. MaterSci Eng, 2000; 291A: 131 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|