| AZ91D镁合金近液相线铸造研究 |
| 乐启炽 欧鹏 |
| 东北大学材料电磁过程研究教育部重点实验到;沈阳110004 |
|
引用本文:
乐启炽; 欧鹏 . AZ91D镁合金近液相线铸造研究[J]. 金属学报, 2002, 38(2): 219-224 .
[1] Luo A, Renaud J, Nakatsugawa I, Plourde J. JOM, 1995;47 (7): 28 [2] Magers D. JOM 1995; 47(7): 26 [3] Demmier A. Europe's automotive components buszness,1997; (1):102 [4] Spencer D B. Mehrabian R, Flemings M C. Metall Trans,1972; 3: 1925 [5] Nussbaum A I. Light Met Age, 1996; (6): 6 [6] Flemings M C. 6th Inter Conf on Semi-Solid Processingof Alloys and Composites, Italy, 2000: Sept. 27-29; 11 [7] Kenney M P, Courtois J A, Evans R D, Farrior G M, Ky-onka C P, Koch A A, Young K P. Metals Handbook, ASMInt, Metals Park, OH, 1988; 15: 327 [8] Zhang K, Liu G J, Xu J, Shi L K. Chln J NonferrousMetall, 2000; 10(1): 47 (张奎,刘国钧,涂 骏,石力开. 中国有色金属学报、2000;10(1):47) [9] Charles V. Metall Trans B, 1992; 23B(4): 189 [10] Osawa Y, Takamori S, Arakane G, Umezawa O, Sato A,Ohashi O. Foundry, 2000; 72(3): 187 (大泽嘉昭.高森 晋.荒金吾郎、梅译 修.佐藤 彰,大桥 修. 铸造工学,2000; 72(3):187) [11] Young K P, Kyonka C P, Courtois J A. US Patent, US 4,415, 374,1983 [12] Robert M H. Trans Jpn Foundrymen's Soc. 1993; 12: 45 [13] Wan G, Witulski T, Hirt G. Metall Ital, 1994; 86: 29 [14] Xia K, Tausig G. Mater Sci Ang, 1998; A246: 1 [15] Hitomi T, Yuasa A, Kamado S, Kojima Y. Jpn Inst LightMet, 1992, 42: 504 (人见高久,由浅 明,镰土重晴.小岛 阳,轻金属.1992;42:504) [16] Kamado S, Yuasa A, Hitomi T, Kojima Y. Jpn Inst LightMet. 1992, 42: 734 (镰土重晴,由浅 明,人见高久,小岛 阳.轻金属,1992;42:734) [17] Sekihara K, Ohnishi S, Kamado S, Kojima Y. Jpn InstLiqht Met, 1995; 45: 516 (关原一敏,大西 智,镰土重晴,小岛 阳. 轻金属,1995;45:516) [18] Sekihara K, Ohnishi S, Kamado S, Kojima Y. Jpn InstLight Met, 1995; 45: 560 (关原一敏,大西 智,镰土重晴,小岛 阳, 轻金属,1995;45: 560) [19] Matsui S, Sekihara K, Kamado S, Kojima Y. Jpn InstLight Met, 1995; 45: 15 (松井伸司,关原一敏,镰土重晴,小岛 阳. 轻金属,1995;45:15) [20] Ohnishi S, Hirata K, Kamado S, Kojima Y.Jpn Inst LightMet, 1996; 46: 644 (大西 智,平田幸四郎,镰土重晴,小岛 阳. 轻金属,1996;46:644) [21] Hirata K, Fufuike W, Rudi R S, Kamado S, Kojima Y.Jpn Inst Liqht Met, 1997; 47: 672 (平田幸四郎,福池 涉,Rudi R S,镰土重晴,小岛 阳.轻金属,1997;47: 672) [22] Polzinger R, Kaufmann H, Uggowitzer P J. In: Chiar-maetta G L, Rosso M eds, 6th Inter Conf on Semi-Solid Processing of Alloys and Composites, Turin, Italy:Edimet Spa-Via Corfu 102, 2000: Sept, 27-29; 85 [23] Wagener W, Hartmann D. In: Chiarmaetta G L, RossoM eds, 6th Inter Conf on Semi-Solid Processing of Alloysand Compositer, Italy: Edimet Spa-Via Corfu 102, 2000:Sept. 27-29; 301 [24] Gebelin J C, Suery M, Favier D. Mater Sci Eng, 1999;A272: 134 [25] Tissier A, Apelian D. J Mater Sci, 1990; 25: 1184 [26] A Ohno. Solidification of Metals. Tiba: Qiyin Publica-tion, 1977; 101: 69 (大野笃美 .金属凝固学,千叶:地人书馆,1977;101:69) [27] Le Q C, Cui J Z. Light Alloy Fabr Technol, 1997; 25(4):14 (乐启炽,崔建忠,轻合金加工技术,1997;25(4):14) [28] Zhang S C, Duan H Q, Cai Q Z, Wei B K, Lin H T. SpecFoundry Nonferrous, 2000; (6): 51 (张诗昌,段汉桥,蔡启舟,魏伯康,林汉同. 特种铸造及有色合金,2000;(6):51) [29] Akiyama S, Ueno I, Sakamoto M, Hirai S, Hokumoto Z.Mate R Jpn, 2000; 39(1): 72 (秋山 茂,上野英俊,坂本 满,平井寿敏,北原 晃.,2000:39(1):72) [30] Chandran R, Sakai T, Kamado S, Kojima Y, MatsuzawaK. J Jpn Inst Light Met, 1998; 48: 13 [31] Zheng L S. Casting alloy and its Smelting. Xi'an: North-western University Press, 1994: 163 (郑来苏,铸造合金及其熔炼.西安:西北工业大学出版社,1994:163) [32] Dong J. M S Dissertation, Northeastern University, 2001 (董 杰 .东北大学硕士论文,2001:21) [33] Kurz W, Fisher D J. Fundamentals of Solidification.Switzerland: Trans Tech Publ. 1984: 22 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|