| bcc-Fe等温压缩下相变的微观模拟与分析 |
| 邵建立;秦承森;王裴 |
| 北京应用物理与计算数学研究所 |
|
| SIMULATIONS AND ANALYSIS OF PHASE TRANSFORMATIONS IN bcc-Fe UNDER ISOTHERMAL COMPRESSION |
| ;; |
| 北京应用物理与计算数学研究所 |
引用本文:
邵建立; 秦承森; 王裴 . bcc-Fe等温压缩下相变的微观模拟与分析[J]. 金属学报, 2008, 44(9): 1085-1089 .
[1]Bancroft D,Peterson E L,Minshall S.J App Phys,1956; 27:291 [2]Johnson P C,Stein B A,Davis R S.J Appl Phys,1962; 33:557 [3]Takahashi T,Bassett W A.Science,1964;145:483 [4]Barker L M,Hollenbach R E.J Appl Phys,1974;45:4872 [5]Taylor R D,Pasternak M P,Jeanloz R.J Appl Phys,1991; 69:6126 [6]Boettger J C,Wallace D C.Phys Rev,1997;55B:2840 [7]Yano K,Horie Y.Int J Plast,2002;18:1427 [8]Caspersen K J,Lew A,Ortiz M,Carter E A.Phys Rev Left,2004;93:115501 [9]Daw M S,Baskes M I.Phys Rev,1984;29B:6443 [10]Finnis M W,Sinclair J E.Philos Mag,1984;50A:45 [11]Kadau K,Germann T C,Lomdahl P S,Holian B L.Sci- ence,2002;296:1681 [12]Kadau K,Germann T C,Lomdahl P S,Holian B L.Phys Rev,2005;72B:064120 [13]Shao J L,Wang P,Qin C S,Zhou H Q.Acta Phys Sin, 2007;56:5389 (邵建立,王裴,秦承森,周洪强.物理学报,2007;56:5389) [14]Shao J L,Wang P,Qin C S,Zhou H Q.Acta Phys Sin, 2008;57:1254 (邵建立,王裴,秦承森,周洪强.物理学报,2008;57:1254) [15]Harrison R J,Voter A F,Chen S P.Atomistic Simulation of Materials Beyond Pair Potentials.New York:Plenum Press,1989:219 [16]Rose J H,Smith J R,Guinea F,Ferrante J.Phys Rev, 1984;29B:2963 [17]Hoffmann K H,Schreiber M.Computational Physics. Berlin:Springer-Verlag,1996:268 [18]Swope W C,Andersen H C,Berens P H,Wilson K R.J Chem Phys,1982;76:637 [19]Irving J H,Kirkwood J G.J Chem Phys,1950;18:817 [20]Allen M P,Tildesley D J.Computer Simulation of Liquids. Oxford:Clarendon Press,1987:46 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|