| 氢对不锈钢纳米压痕蠕变的影响 |
| 郜 欣; 乔利杰; 宿彦京; 褚武扬 |
| 北京科技大学材料物理系; 北京 100083 |
|
| Effect Of Hydrogen On Nanoindentation Creep Of Type 316 Stainless Steel |
| GAO Xin; QIAO Lijie; SU Yanjing; CHU Wuyang |
| Department of Materials Physics; University of Science and Technology Beijing; Beijing 100083 |
引用本文:
郜欣; 乔利杰; 宿彦京; 褚武扬 . 氢对不锈钢纳米压痕蠕变的影响[J]. 金属学报, 2005, 41(4): 342-346 .
,
,
,
.
Effect Of Hydrogen On Nanoindentation Creep Of Type 316 Stainless Steel[J]. Acta Metall Sin, 2005, 41(4): 342-346 .
[1]Cornet M, Talbat-Besnard S. Suppl Trans JIM, 1980; 21: 545 [2]Gao G Y, Dexter S C. Metall Trans A, 1987; 18A: 1125 [3]Chu W Y, Ding W, Hsiao C M. Ada Metall Sin, 1986; 22: 115 (褚武扬,丁威,肖纪美.金属学报, 1986;22:115) [4]Gao B, Chu W Y, Qiao L J.Carros Sci, 1994; 36: 1437 [5]Abraham D P, Altstetter C J. Metall Mater Trans A, 1995; 26A: 2849 [6]Birnhaum H K, Sofronis P. Mater Sci Eng, 1994; A176: 191 [7]Chen J, Wang W, Lu L, Lu K. Acta Metall Sin, 2001; 37: 1179 (陈吉,汪伟,卢磊,卢柯.金属学报,2001;37: 1179) [8]Chudoha T, Richter F. Surf Coat Technol, 2001; 148: 191 [9]Ma X, Yoshida F. Appl Phys Lett, 2003; 82: 188 [10]Feng G, Ngan A H W. Scr Mater, 2001; 45: 971 [11]Yao Y, Qiao L J, Sun D B, Chu W Y. Acta Metall Sin, 2003; 39: 855 (姚远,乔利杰,孙冬柏,褚武扬.金属学报,2003;39:855) [12]Li W B, Henshall J L, Hovper R M, Easterling K E. Acta Metall Mater, 1991; 39: 3099 [13]Chu W Y, Qiao L J, Chen Q Z, Gao K W. Fracture and Environmental Fracture. Beijing: Science Press, 2000: 112 (褚武扬,乔利杰,陈奇志,高克玮.断裂与环境断裂.北京: 科学出版社,2001:112) [14]Li J C M, Park C G, Ohr S M. Scr Metall, 1986; 20: B447 [15]Wang Y B, Chu W Y, Hsiao C M. Scr Metall, 1985; 19: 1161 [16]Zhang T Y, Chu W Y, Hsiao C M. Scr Metall, 1986; 20: 225 [17]Birnhanm H K, Sofronis P. Mater Sci Eng, 1994; A176: 191 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|