| 铝合金三维枝晶生长相场模拟 |
| 赵红兆 荆 涛 柳百成 |
| 清华大学机械工程系; 北京 100084 |
|
引用本文:
赵红兆; 荆涛; 柳百成 . 铝合金三维枝晶生长相场模拟[J]. 金属学报, 2005, 41(5): 491-495 .
[1] Kobayashi R. Phys, 1993; 63D: 410 [2] Karma A, Rappel W J. Phys Rev, 1999; 60E: 3614 [3] Karma A, Rappel W J. Phys Rev Lett, 1996; 77: 4050 [4] Karma A, Rappel W J. J Cryst Growth, 1997; 174: 54 [5] Karma A, Rappel W J. Phys Rev, 1998; 57E: 4323 [6] Tiaden J, Nestler B, Diepers H J, Steinbach I. Phys, 1998; 115D: 73 [7] Zhao D P, Jing T. Acta Metall Sin, 2002; 38: 1238 (赵代平,荆涛.金属学报,2002;38:1238) [8] Diepers H J, Beckermann C, Steinbach I. Acta Mater, 1999; 47: 3663 |
|