| Ca-Tb4O7-Fe体系的热力学研究 |
| 郭广思 隋智通 周玉林 |
| 东北大学材料与冶金学院;沈阳110006 |
|
引用本文:
郭广思; 隋智通; 周玉林 . Ca-Tb4O7-Fe体系的热力学研究[J]. 金属学报, 2001, 37(2): 189-192 .
[1] Ying Q M, Luo Z X, Li D P, Wang R K, Yao G Q, Ren SK, Zhang J, Zhang L H. Rare-Earth, 1999; 20: 72(应启明, 罗梓贤, 李东培, 王瑞坤, 姚国庆, 任世宽, 健,张丽红. 稀土, 1999; 20: 72) [2] Xu G X. Rare-Earth. 3rd Book, Beijing: Metallurgy Industry Press, 1995: 102(徐光宪主编. 稀土. 下册, 北京: 冶金工业出版社, 1995: 102) [3] Qi G J, Hino M, Yaxawa A. Mater Trans JIM, 1990: 31:463 [4] Song C, Ogawa O. J Min Mater Proc Inst, 1996; 110: 487 [5] Niessen A K, de Boer F R, Boom R, de Chatel P F, Mattens W C M, Miedema A R. CALPHAD, 1983; 7: 51 [6] Liang Y J, Che Y C. Hand Book of ThermodynamicalData for Inorganic Substance. Shenyang: NortheasternUniversity Press, 1993: 514(梁英教, 车荫昌. 无机物热力学数据手册. 沈阳: 东北大学出版社, 1993: 514) |
|