					引用本文:
						|  |  
    					|  |  
    					| 包晶合金定向凝固平界面前沿的形核分析 |  
						| 李双明;刘林;李晓历;傅恒志 |  
					| 西北工业大学凝固技术国家重点实验室 |  
						|  |  
    					| Nucleation At Plane Front In Directionally Solidified Peritectic Alloys |  
						| LI Shuangming; LIU Lin; LI Xiaoli; FU Hengzhi |  
						| State Key Laboratory of Solidification Processing; Northwestern Polytechnical University |  
								李双明; 刘林; 李晓历; 傅恒志                                                                                                                                                                                                                                      . 包晶合金定向凝固平界面前沿的形核分析[J]. 金属学报, 2004, 40(1): 20-26        .	
																												,
																								 ,
																								 ,
																												 . 
				Nucleation At Plane Front In Directionally Solidified Peritectic Alloys[J]. Acta Metall Sin, 2004, 40(1): 20-26        .
 
					
						| 
								
									|  
          
          
            
                         
            
									            
									                
																														  
																| [1] Kerr H W, Kurz W. Inter Mater Rev, 1996; 41:129 [2] Barker N J W, Hellawell A. Metal Sci, 1974; 8:353
 [3] Brody H D, David S A. Int Conf on Solidification and Casting, Institute of Metals, London, 1977:144
 [4] Tichener A P, Spittle J A. Acta Metall, 1975; 23:497
 [5] Ostowski A, Langer E W. Int Conf on Solidification and Casting, Institute of Metals, London, 1977:139
 [6] Boettinger W J. Metall Trans, 1974; 5:2203
 [7] Trivedi R. Metall Mater Trans, 1995; 26A: 1583
 [8] Zeissler M K, Lograsso T. Metall Mater Trans, 1997; 28A: 1543
 [9] Kurz W, Trivedi R. Metall Mater Trans, 1996; 27A: 625
 [10] Tokieda K, Yasuda H, Ohnaka I. Mater Sci Eng, 1999; A262:241
 [11] Karma A, Rappel W J, Fuh B C, Trivedi R. Metall Mater Trans, 1998; 29A: 1457
 [12] Trivedi R, Park J S. J Cryst Growth, 2002; 235:572
 [13] Hunziker O, Vandyoussefi M. Kurz W. Acta Mater, 1998; 46:6325
 [14] Tiller W A. The Science of Crystallization: Macroscopic Phenomena and Defect Generation. Cambribge: Cambridge University Press, 1991:143
 [15] Hu H Q. Solidification Principle of Metals. The 2nd edition. Beijing: Machinary Industry Press, 2000:114(胡汉起.金属凝固原理.第2版,北京:机械工业出版社,2000:114)
 [16] Umeda T. Okane T, Kurz W. Acta Mater, 1996; 44:4214
 [17] Umeda T, Okane T. Sci Technol Adv Mater, 2001; 2:239
 |  
             
												
											    	
											        	|  | Viewed |  
											        	|  |  |  
												        |  | Full text 
 | 
 
 |  
												        |  |  |  
												        |  | Abstract 
 | 
 |  
												        |  |  |  
												        |  | Cited |  |  
												        |  |  |  |  
													    |  | Shared |  |  
													    |  |  |  |  
													    |  | Discussed |  |  |  |  |