| Cu-Nu-Ti合金钎料对Si3N4陶瓷的润湿与连接 |
| 熊华平 万传庚 周振丰 |
| 吉林工业大学材料科学与工程学院; 长春 130025 |
|
引用本文:
熊华平; 万传庚; 周振丰 . Cu-Nu-Ti合金钎料对Si3N4陶瓷的润湿与连接[J]. 金属学报, 1999, 35(5): 527-530 .
[1] Bac F H, Ren J L, Zhou Y H. fons China Weld lust, 1990;11: 200(包芳涵,任家烈,周运鸿,焊接学报,1990; 11: 200) [2] Xian A P, St Z Y. i Mater Set, 1990; 25: 4483 [3] Katayama K. SAE 861128, 1986 [4] Naka M, Kubo M. Trans JWRI, 1987; 16(1): 83 [5] Nabal M, Kubo M. J Mater Set, 1987; 22: 4417 [6] Naka M, Kubo M. bons JWRI, 1990; 19(2): 21 [7] Naka M, Kubo M. Trans JWRI, 1990; 19(1): 25 [8] Yu J Q I Yi W Z I Chen B D, Chen H J. The Collectionof Phase Diagrums of Binary Alloys. Shanghai: ShanghaiScience and Technology Press, 1983: 350(虞觉奇,易文质,陈帮迪,陈宏鉴.二元合金壮态图集.上海上海科学技术出版社,1983: 350) [9] Miedema A R, Boer F R, Boom R, Dorleijn J W F. Calphad,1977; 1: 353 [10] Klomp J T. Joining Of Ceramics. London: Champman &Hall, 1990: 113 [11] Nishino T, Urai S, Okamoto I, Naka M. Weld nit, 1992; 6:600 |
|