| 激光熔覆溶池二维准稳态流场及温度场的数值模拟 |
| 曾大文 谢长生 |
| 华中理工大学国家模具技术重点实验室; 武汉 430074 |
|
引用本文:
曾大文; 谢长生 . 激光熔覆溶池二维准稳态流场及温度场的数值模拟[J]. 金属学报, 1999, 35(6): 604-610 .
[1]Wang A H, Tho Z Y, Zhu B T. Weld J, 1991; 70(4): 106 [2]Volz R, Battling K. ICALEO, 1993: 999 [3]Oilier B, pirch N, Kreutz E W. Laser Optoelectronics, 1996;1(1):8 [4]Picasso M, Hoadley A F A. Int J Meth Heat Fluid Flow,1994; 4:61 [5]Lai H X.Ph D thesis, Huazhong University of Science and Technology, 1997 [6]Rieger H, Projhan U, Beer H, Numer Heat Transfer, 1983; 6:1 [7]Cheng H P,Zheq X H,In:Symposium of Heat and Mass Transfer ed.,ASolution of Convection-Diffusion Problem in the Orthogonal Curvilinear Coordinates with Complex Ge ography. Beijing: Academy of Engineering Thermophysics,1987, 973230 [8]Xiong C X, Xu J Z.J he Thermophys, 1993; 14(1): 24 [9]Tao W Q. Numerical Heat Transfer. Xi’an: Published by Xi’an Jiaotong University, 1988:541 [10]Harlow F H, Welch J E. Phys Fluids, 1965;(8): 2182 [11]Rhie C M; Chow W L. AIAA, 1983; 21: 21525 [12]Zeng X Y,Zhu B D,Tao Z Y.Chin Laser ,1993;20:211 [13]Zeng D W, Wang M Q, Xie C S. Rare Metal Mater Eng,1998;27:87L |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|